| DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY |
| Niu E |
| 北京科技大学材料物理系 |
|
Cite this article:
Niu E. DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY. Acta Metall Sin, 2006, 42(4): 369-373 .
|
|
|
Abstract In situ observation of delayed propagation of unloaded indentation crack in humid air, as well as delayed domain change and delayed cracking induced by constant magnetic field in humid air for (Tb,Dy)Fe2 magnetostrictive alloy have been investigated using differential inference contrast microscope. The results showed that a residual stress during indenting could cause delayed propagation of unloaded indentation crack in humid air. A magnetic field exceeded a threshold field Hth caused instant propagation of indentation crack. A constant magnetic field below Hth could cause delayed change of domain configuration in humid air and delayed propagation of indentation crack in humid air.
|
|
Received: 08 August 2005
|
|
|
[1] Engdahl G. In: Mayergoyz I ed, Handbook of Giant Mag-netostrictive Materials, New York: Academic Press, 2000: 1 [2] Wang B W. Preparation and Devices Design of Giant Magnetostrictive Materials. Beijing: Metallurgical Industry Press, 2003 (王博文.超磁致伸缩材料制备与器件设计.北京:冶金工业出 版社, 2003) [3] Wang B W, Yan R G. J Hebei Univ Technol, 2004; 33(2): 16 (王博文,闫荣格.河北工业大学学报, 2004;33(2):16) [4] Li K S, Li H W, Fang Y K. J Rare Earths, 2004; 22: 126 [5] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B59: 263 [6] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. J Appl Phys, 2003; 82: 1583 [7] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 14 (杨 卫.力电失效学.北京:清华大学出版社, 2001:14) [8] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811 [9] Wang R M, Chu W Y, Su Y J, Gao K W, Qiao L J. Acta Metall Sin, 2005; 41: 297 (王瑞敏,褚武扬,宿彦京,高克玮,乔利杰.金属学报,2005; 41:297) [10] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 6 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京: 科学出版社,2000:6) [11] Anstis G R, Chantikul P, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 533 [12] Chantikul P, Anstis G R, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 539 [13] Ma R Z, Jiang M H, Xu Z X. Functional Materials Generality. Beijing: Metallurgical Industry Press, 1999: 80 (马如璋,蒋民华,徐祖雄.功能材料学概论.北京:冶金工业 出版社,1999:80) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|