DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY
Niu E
北京科技大学材料物理系
Cite this article: 

Niu E. DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY. Acta Metall Sin, 2006, 42(4): 369-373 .

Download:  PDF(867KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In situ observation of delayed propagation of unloaded indentation crack in humid air, as well as delayed domain change and delayed cracking induced by constant magnetic field in humid air for (Tb,Dy)Fe2 magnetostrictive alloy have been investigated using differential inference contrast microscope. The results showed that a residual stress during indenting could cause delayed propagation of unloaded indentation crack in humid air. A magnetic field exceeded a threshold field Hth caused instant propagation of indentation crack. A constant magnetic field below Hth could cause delayed change of domain configuration in humid air and delayed propagation of indentation crack in humid air.
Key words:  (Tb      Dy)Fe2      constant magnetic field      domain change      delayed cracking      
Received:  08 August 2005     
ZTFLH:  TG111.91  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I4/369

[1] Engdahl G. In: Mayergoyz I ed, Handbook of Giant Mag-netostrictive Materials, New York: Academic Press, 2000: 1
[2] Wang B W. Preparation and Devices Design of Giant Magnetostrictive Materials. Beijing: Metallurgical Industry Press, 2003 (王博文.超磁致伸缩材料制备与器件设计.北京:冶金工业出 版社, 2003)
[3] Wang B W, Yan R G. J Hebei Univ Technol, 2004; 33(2): 16 (王博文,闫荣格.河北工业大学学报, 2004;33(2):16)
[4] Li K S, Li H W, Fang Y K. J Rare Earths, 2004; 22: 126
[5] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B59: 263
[6] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. J Appl Phys, 2003; 82: 1583
[7] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 14 (杨 卫.力电失效学.北京:清华大学出版社, 2001:14)
[8] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811
[9] Wang R M, Chu W Y, Su Y J, Gao K W, Qiao L J. Acta Metall Sin, 2005; 41: 297 (王瑞敏,褚武扬,宿彦京,高克玮,乔利杰.金属学报,2005; 41:297)
[10] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 6 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京: 科学出版社,2000:6)
[11] Anstis G R, Chantikul P, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 533
[12] Chantikul P, Anstis G R, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 539
[13] Ma R Z, Jiang M H, Xu Z X. Functional Materials Generality. Beijing: Metallurgical Industry Press, 1999: 80 (马如璋,蒋民华,徐祖雄.功能材料学概论.北京:冶金工业 出版社,1999:80)
[1] . Research Of Flaking And Its Fractography In A Wheel Steel[J]. 金属学报, 2006, 42(3): 273-279 .
[2] Xuechong Ren. Effects of Atomic Hydrogen and Flaking on Mechanical Properties of Wheel Steel[J]. 金属学报, 2006, 42(2): 153-157 .
[3] CHEN Liqiang; GONG Shengkai; XU Huibin. INFLUENCE OF VERTICAL CRACKS ON FAILURE MECHANISM OF EB-PVD THERMAL BARRIER COATINGS DURING THERMAL CYCLING[J]. 金属学报, 2005, 41(9): 979-984 .
[4] ZHOU Bangxin;ZHENG Sikui;WANG Shunxin Southwest Centre for Nuclear Reactor Engineering Research and Design Chengdu. IN SITU ELECTRON MICROSCOPY STUDY ON PRECIPITATION OF ZIRCONIUM HYDRIDES INDUCED BY STRAIN AND STRESS IN ZIRCALOY-2[J]. 金属学报, 1989, 25(3): 34-39.
No Suggested Reading articles found!