THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS
daitiejun
Cite this article: 

daitiejun. THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS. Acta Metall Sin, 2006, 42(3): 280-284 .

Download:  PDF(177KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the concept of iron-flow diagram of steel production process, a relational expression between iron resource efficiency of steel production process and of its unit process has been derived. By using the data of a steel plant, the relationship between iron resource efficiency of steel production process and of its unit process was analyzed, and the influence of iron resource efficiency of unit process on iron resource efficiency of steel production process was discussed as examples.
Key words:       
Received:  30 August 2005     
ZTFLH:  TF089  
  F205  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I3/280

[1]Zhang S R.Res Iron Steel,2002;30(2):1 (张寿荣.钢铁研究,2002;30(2):1)
[2] Zhang X Y.Metall Manag,2003;(8):14 (张训毅.冶金管理, 2003;(8):14)
[3] Chen J B. Geol Seek, 2004; 19(1): 5 (陈甲斌.地质找矿论丛, 2004;19(1):5)
[4] Kleijn R. J Ind Ecol, 1999; 3(2, 3): 8
[5] Ayres R U. Resour Conseru Recycling, 1997; 21: 145
[6] Huang S L, Hsu W L. Landscape Urban Plann, 2003; 63: 61
[7] Fischer-Kowalski M. J Ind Ecol, 1998; 2(1): 61
[8] Fischer-Kowalski M, Hyttler W. J Ind Ecol, 1998; 2(4): 107
[9] de Marco O, Lagioia G, Mazzacane E P. J Ind Ecol , 2000; 4(2): 55
[10] Maenpaa I, Juutinen A. J Ind Ecol, 2001; 5(1): 33
[11] Spatari S, Bertram M, Fuse A K, Graedel T E, Rechberger H. Ecol Econo, 2002; 42: 27
[12] Hekkert M P, Joosten L A J, Worrell E. Resour Conser Recycling, 2000; 30: 29
[13] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 131
[14] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 209
[15] Yin R Y. Metallurgical Process Engineering. Beijing: Metallurgical Industry Press, 2004: 115 (殷瑞钰.冶金流程工程学.北京:冶金工业出版社,2004:115)
[16] Lu Z W, Cai J J, Yu Q B, Xie A G. Acta Metall Sin, 2000; 36: 370 (陆钟武,蔡九菊,于庆波,谢安国.金属学报,2000;36:370)
[17] Lu Z W. Acta Metall Sin, 2002; 38: 58 (陆钟武.金属学报,2002;38:58)
[18] Lu Z W, Dai T J. Iron Steel, 2005; 40(4): 1 (陆钟武,戴铁军.钢铁,2005;40(4):1)
[19] Dai T J, Lu Z W. Acta Metall Sin, 2004; 40: 1127 (戴铁军,陆钟武.金属学报,2004;40:1127)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!