| Diffusion-induced Stresses |
|
Cite this article:
. Diffusion-induced Stresses. Acta Metall Sin, 2006, 42(3): 225-233 .
|
|
|
Abstract Recent experiments indicate that stresses induced by atomic interdiffusion in solids can not only result in the macro-distortion of materials, but also form some peculiar micro-structures in the materials. Considered that little has been known in a detailed way of the mechanisms of diffusion-induced stresses, the relationship of atomic diffusion and stresses in solids will be elucidated and the concepts of creep-induced diffusion and diffusion-induced stresses are clarified in this paper. Based on the volume growth rate of a flow point, an equation is obtained for the relationship of stresses of flow point and atomic diffusion fluxes and therefore a general theory is constructed to describe the phenomena of diffusion-induced stresses and strains, e.g. the bending of thin diffusion couples and the periodic layer formation during solid state reactions.
|
|
Received: 07 June 2005
|
|
|
[1] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2004; A368: 1 [2] Daruka I, Szabo I A, Beke D L, Cserhati Cs, Kodentsov A, van Loo F J J. Acta Mater, 1996; 44: 4981 [3] Szabo I A, Daruka I, Beke D L. Defect Diffus Forum, 1996; 129/130: 127 [4] Greer A L, Karpe N, Bottinger J. J Alloys Compd, 1993; 194: 199 [5] Bastin G F, Rieck G D. Metall Trans, 1974; 5: 1817 [6] Osinski K, Vriend A W, Bastin G F, van Loo F J J. Z Metallkd, 1982; 73: 258 [7] Kodentsov A A, Rijnders M R, van Loo F J J. Acta Mater, 1998; 46: 6521 [8] Philibert J. Defect Diffus Forum, 1996; 129/130: 3 [9] d'Heurle F M, Gas P, Philibert J, Zhang S L. Defect Diffus Forum, 2001; 194/199: 1631 [10] Xia S W. Active Energy and Its Calculation. Beijing: Higher Education Press, 1993 (夏少武.活化能及其计算.北京:高等教育出版社, 1993) [11] Mehrer H. Defect Diffus Forum, 1996; 129/130: 57 [12] Lin D L. Crystal Defects. Shanghai: Shanghai Jiaotong University Press, 1996 (林栋梁.晶体缺陷.上海:上海交通大学出版社, 1996) [13] Huang J H. Diffusion in Metals and Alloys. Beijing: Metallurgical Industry Press, 1996 (黄继华.金属及合金中的扩散.北京:冶金工业出版社,1996) [14] Kraftmakher Y. Defect Diffus Forum, 2001; 194/199: 23 [15] Gutmann A M, Translated by Jin S. Mechanical Chem- istry and Corrosion Protection of Metals. Beijing: Science Press, 1989 (Gutmann A M著,金 石译.金属力学化学与腐蚀防护.北 京:科学出版社,1989) [16] Oikawa H, Landon T G. In: Evans R W, Wilshire B, eds., Creep of Metals and Alloys, London: The Institute of Metals, 1985 [17] Poirier J P. Creep of Crystals. Cambridge: Cambridge University Press, 1985 [18] Oikawa H, Landon T G. In: Wilshire B, Evans R W, eds., Creep Behaviour of Crystalline Solids, Swansea: Piner- idge Press, 1985 [19] Kraftmakher Y. Phys Rep, 1998; 299: 79 [20] Yu Z H, Miao M Q, Jiang Q R, Yang P Z. Fluid Mechanics. The Revised Edition, Beijing: Meteorology Press, 1994 (余志豪,苗曼倩,蒋全荣,杨平章.流体力学.修订版,北京: 气象出版社,1994) [21] Xu Z L. Elasticity Mechanics. Beijing: People's Education Press, 1979 (徐芝纶.弹性力学.北京:人民教育出版社, 1979) [22] Poirier J P, translated by Wang G X. Plasticity of Crystalline Materials at High Temperatures. Taibei: Quanhua Science Book Company, 1978 (Poirier J P著,王恭心编译.晶体高温塑性学.台北:全华科 技图书股份有限公司, 1978) [23] Rapp R A, Ezis A, Yurek G J. Metall Trans, 1973; 4: 1283 [24] Markovski S L, van Dal M J H, Verbeek M J L, Kodentsov A A, van Loo F J J. J Phase Equilib, 1999; 20: 373 [25] Chen Y C, Qi L, Zhang Y G, Chen C Q. Ada Metall Sin, 2005; 41: 235 (陈永翀,其鲁,张永刚,陈昌麒.金属学报,2005;41:235) [26] Rijnders M R, Kodentsov A A, Cserhati Cs, van den Akker J, van Loo F J J. Defect Diffus Forum, 1996; 129/130: 253 [27] Liu H W. Materials Mechanics. 3rd Ed., Beijing: Higher Education Press, 1992 (刘鸿文.材料力学.第3版,北京:高等教育出版社,1992) [28] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2004; A362: 135 [29] Greer A L. Defect Diffus Forum, 1996; 129/130: 339 [30] Kodentsov A A, van Dal M J H, Cserhati Cs, Gusak A M, van Loo F J J. Defect Diffus Forum, 2001; 194/199: 1491 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|