| Effects of Electric Field Annealing on the Recrystallization Texture of Cold Rolled 08Al Killed Steel Sheet |
| HU Zuochao; ZHAO Xiang; ZUO Liang |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110004 |
|
Cite this article:
HU Zuochao; ZHAO Xiang; ZUO Liang. Effects of Electric Field Annealing on the Recrystallization Texture of Cold Rolled 08Al Killed Steel Sheet. Acta Metall Sin, 2003, 39(2): 213-216 .
[1] Schmid E. Boas W. Plasticity of Crystals. Landau: Cha-mpan and Hall, 1968: 104 [2] Hav R K. Jonas J J, Hook R E. Int Met Rev, 1994; 39:129 [3] Blickwede D J. Trans ASM, 1968; 61: 462 [4] Ray R K. Jonas J J. Int Met Rev, 1990; 35: 1 [5] Conrad H, Cao W D, Sprecher A F. Scr Metatl Mater,1989: 23: 821 [6] Sprecher A F, S. Mannan L, Conrad H. Ada Metall, 1986;34: 1145 [7] Koch C C. Mater Sci Eng, 2000; A287: 213 [8] Liang Z D, Xu J Z, Wang F. 3-D Orientation DistributionAnalysis of Textured Materials. Shenyang: NortheasternUniversity of Technology Press, 1986: 108(梁志德,徐家祯,王福,织构材料的三维取向分析术-ODF分析,沈阳:东北工学院出版社, 1986:108) [9] Jonas J J, Urabe T. Proc Int Forum on Physical Metallurgy of IF Steel. Tokyo, ISIJ, 1994: 77 [10] Kuhotera H, Nakaoka K, Araki K, Watanabe K Nishi-moto A, Iwase K. Tetsu Hagane, 1976: 62: 624(久保寺治朗,中(?)一秀,荒木 健治,渡边馨,西本 昭彦,岩濑耕二铁 钢,1976;62:624) [11] Hutchinson W B. Watson T W, Dillamore I L. J Iron SteelInst (London), 1969; 207: 1479 [12] Vatne H E, Daaland O. Mater Sci Forum, 1994; 157-162:1087 [13] Baluffi R W. Grain Boundary Structure and Kinetics.Metals Park. Ohio: ASM, 1979: 125o |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|