Effects of Electric Field Annealing on the Recrystallization Texture of Cold Rolled 08Al Killed Steel Sheet
HU Zuochao; ZHAO Xiang; ZUO Liang
School of Materials and Metallurgy; Northeastern University; Shenyang 110004
Cite this article: 

HU Zuochao; ZHAO Xiang; ZUO Liang. Effects of Electric Field Annealing on the Recrystallization Texture of Cold Rolled 08Al Killed Steel Sheet. Acta Metall Sin, 2003, 39(2): 213-216 .

Download:  PDF(158KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  17 April 2002     
ZTFLH:  TG115.23  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I2/213

[1] Schmid E. Boas W. Plasticity of Crystals. Landau: Cha-mpan and Hall, 1968: 104
[2] Hav R K. Jonas J J, Hook R E. Int Met Rev, 1994; 39:129
[3] Blickwede D J. Trans ASM, 1968; 61: 462
[4] Ray R K. Jonas J J. Int Met Rev, 1990; 35: 1
[5] Conrad H, Cao W D, Sprecher A F. Scr Metatl Mater,1989: 23: 821
[6] Sprecher A F, S. Mannan L, Conrad H. Ada Metall, 1986;34: 1145
[7] Koch C C. Mater Sci Eng, 2000; A287: 213
[8] Liang Z D, Xu J Z, Wang F. 3-D Orientation DistributionAnalysis of Textured Materials. Shenyang: NortheasternUniversity of Technology Press, 1986: 108(梁志德,徐家祯,王福,织构材料的三维取向分析术-ODF分析,沈阳:东北工学院出版社, 1986:108)
[9] Jonas J J, Urabe T. Proc Int Forum on Physical Metallurgy of IF Steel. Tokyo, ISIJ, 1994: 77
[10] Kuhotera H, Nakaoka K, Araki K, Watanabe K Nishi-moto A, Iwase K. Tetsu Hagane, 1976: 62: 624(久保寺治朗,中(?)一秀,荒木 健治,渡边馨,西本 昭彦,岩濑耕二铁 钢,1976;62:624)
[11] Hutchinson W B. Watson T W, Dillamore I L. J Iron SteelInst (London), 1969; 207: 1479
[12] Vatne H E, Daaland O. Mater Sci Forum, 1994; 157-162:1087
[13] Baluffi R W. Grain Boundary Structure and Kinetics.Metals Park. Ohio: ASM, 1979: 125o
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!