Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (1): 87-92     DOI:
Research Articles Current Issue | Archive | Adv Search |
Study on Extraction of Iron by the Short Circuit Reduction Method
GAO Yunming; GUO Xingmin; CHOU Kuochih
Key Laboratory Ferrous Metallargy and Resources Utiliztion; Ministry of Education; Wuhan University of Science and Technology; Wuhan 430081
Cite this article: 

GAO Yunming; GUO Xingmin; CHOU Kuochih. Study on Extraction of Iron by the Short Circuit Reduction Method. Acta Metall Sin, 2006, 42(1): 87-92 .

Download:  PDF(816KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  29 April 2005     
ZTFLH:  TF111.15  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I1/87

[1]Chou K C,Gao Y M,Guo X M,Lu X G,Xu K D.Proceedings of the 10th Japan-China Symposium on Science and Technology of Iron and Steel,Chiba,Japan:The Iron and Steel Institute of Japan,2004:162
[2]Oberg K E,Friedman L M,Boorstein W M,Rapp R A.Metall Trans,1973;4:75
[3]Yuan S,Pal U,Chou K C.J Am Ceram Soc,1996;79:641
[4]Soral P,Pal U,Larson H R,Schroeder B.Metall Mater Trans,1999;30B:307
[5]Hu X J,Xiao L,Li F S,Lu X G,Li L F,Chou K C.Acta Metall Sin,1999;35:316(胡晓军,肖莉,李福燊,鲁雄刚,李丽芬,周国治.金属学报,1999;35:316)
[6]Li F S,Lu X G,Jin C J,Chou K C,Zhu L X,Hu X J,Li Z Y,Wang F,Shen Q.Acta Metall Sin,2003;39:287(李福燊,鲁雄刚,金从进,周国治,朱立新,胡晓军,李泽亚,王峰,沈强.金属学报,2003;39:287)
[7]Li F S,Lu X G,Jin C J,Chou K C,Zhu L X,Hu X J,Li Z Y,Wang F,Shen Q.Acta Metall Sin,2004;40:673
??(李福燊,鲁雄刚,金从进,周国治,朱立新,胡晓军,李泽亚,王峰,沈强.金属学报,2004;40:673)
[8]Lu X G,Liang X W,Yuan W,Sun M S,Ding W Z,Chou K C.Acta Metall Sin,2005;41:113(鲁雄刚,梁小伟,袁威,孙铭山,丁伟中,周国治.金属学报,2005;41:113)
[9]Semkow K W,Sammells A F.J Electrochem Soc,1987;134:2088
[10]Woolley D E,Pal U,Kenney G B.High Temp Mater Processes,2001;20:209
[11]Wang C Z.Research Methods of Physical Chemistry in Metallurgy.Beijing:Metallurgical Industry Press,2002;150(王常珍.冶金物理化学研究方法.北京:冶金工业出版社,2002:150)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!