Effect of Fe3O4 Particles on Thermal Expansion Behavior of Al 18B4O33 Whisker Reinforced Aluminum Composite
LI Gang; SUN Yue; FEI Weidong
School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001
Cite this article: 

LI Gang; SUN Yue; FEI Weidong. Effect of Fe3O4 Particles on Thermal Expansion Behavior of Al 18B4O33 Whisker Reinforced Aluminum Composite. Acta Metall Sin, 2006, 42(1): 83-86 .

Download:  PDF(619KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  07 April 2005     
ZTFLH:  TB33  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I1/83

[1]Arsenault R J,Taya M.Acta Metall,1987;35:651
[2]Arsenault R J,Wu S B.Mater Sci Eng,1987;96:77
[3]Fei W D,Hu M,Yao C K.Mater Chem Phys,2003;77:882
[4]Fei W D,Chu W G,Yang W,Liu Q Y,Yao C K.MaterSci Technol,2000;16:431
[5]Fei W D,Liu Q Y,Liang N G,Yao C K.Mater Sci Technol,2001;17:912
[6]Li G,Sun Y,Fei W D.Mater Lett,2003;57:3217
[7]Levy D,Artioli G,Dapiaggi M.J Solid State Chem,2004;177:1713
[8]Wang L D,Fei W D,Jiang L S,Yao C K.J Mater Sci Lett,2002;21:737
[9]Kim C T,Lee J K,Plichta M R.Metall Trans,1990;21A:673
[10]Maeda K,Wakashima K,Ono M.Scr Mater,1997;36:335
[11]Samara G A,Giardini A A.Phys Rev,1969;186:577
[12]Govindarajan R,Carmichael C M,Schloessin H H.Phys Earth Plan Int,1982;29:108
[13]Jiang S T,Li W.Magnetic Physics of Condensed State(2nd,ed).Beijing:Science Press,2005:55(姜寿亭,李卫.凝聚态磁性物理(第二版).北京:科学出版社,2005:55)
[14]Chaianni A,Yokoya T,Morimoto T,Takahashi T,Todo S.J Electron Spectros Relat Phenom,1996;78:99
[15]Li Y R,Yun Z Z.An Introduction to Electronic Materials.Beijing:Tsinghua University Press,2001:329(李言荣,恽正中.电子材料导论.北京:清华大学出版社,2001:329)
[16]Fei W D,Wang L D.Mater Chem Phys,2004;85:450
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!