Abstract IrO2--Ta2O5 oxide anode was prepared by coating
oxide on titanium substrate which has
been pretreated by sandblast and oxalic acid etching. ESEM,
polarization curve and EIS indicated that the corrosion rate of the
substrate and the loading of the oxide coating (i.e. Ir content)
increase with etching time at the initial stage and then
decrease. The oxide coating
on the substrate pretreated by suitable etching pretreatment is of a
uniform and compact surface which has large electrochemical active
surface area, fine electrocatalytic
activity for oxygen evolution and high stability.
|
|
Received: 04 November 2004
|
|
|
[1] Trasatti S. Electrochim Acta, 2000; 45: 2377 [2] Comninellis Ch, Vercesi G P. J Appl Electrochem, 1991; 21: 335 [3] Rolewicz J, Cominiellis Ch, Plattner E, Hinden J. Elec trochim Acta, 1988; 33: 573 [4] Mraz R, Krysa J. J Appl Electrochem, 1994; 24: 1262 [5] Xu L K, Scantlebury J D. J Electrochem Soc, 2003; 150: B288 [6] Xu L K, Scantlebury J D. J Electrochem Soc, 2003; 150: B254 [7] Martelli G N, Ornelas R, Faita G. Electrochim Acta, 1994; 39: 1551 [8] Krysa J, Kule L, Mraz R, Rousar I. J Appl Electrochem, 1996; 26: 999 [9] Krysa J, Maixner J, Mraz R, Rousar I. J Appl Electrochem, 1998; 28: 369 [10] Krysa J, Mraz R. Electrochim Acta, 1995; 40: 1997 [11] Otogawa R, Morimitsu M, Matsunaga M. Electrochim Acta, 1998; 44: 1509 [12] Hu J M, Meng H M, Zhang J Q, Cao C N. Acta Metall Sin, 2002; 38: 69 (胡吉明,孟惠民,张鉴清,曹楚南.金属学报,2002;38:69) [13] Xu L K, Scantlebury J D. Corros Sci, 2003; 45: 2729 [14] Beck F. Electrochim Acta, 1989; 34: 811 [15] Loucka T. J Appl Electrochem, 1997; 7: 211 [16] Roginskaya Yu E, Morozova O V, Loubnin E N, Popov A V, Ulition Yu I, Zhurov V V, Ivanov S A, Trasatti S. J Chem Soc Faraday Trans, 1993; 89: 1707 [17] Wen T C, Hu C C. J Electrochem Soc, 1992; 139: 2158 [18] Shieh D T, Hwang B J. Electrochim Acta, 1993; 38: 2239 [19] Lassali T A F, Boodts J F C, Bulhoes L O S. Electrochim Acta, 1999; 44: 4203 [20] Hu J M, Meng H M, Zhang J Q, Wu J X, Yang D J, Cao C N. Acta Metall Sin, 2001; 37: 628 (胡吉明,孟惠民,张鉴清,吴继勋,杨德钧,曹楚南,金属学 报,2001;37:628) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|