Acta Metall Sin  2003, Vol. 39 Issue (1): 30-34     DOI:
Research Articles Current Issue | Archive | Adv Search |
Microstructure Characteristics of FGH95 Superalloy Powders Prepared by Prep
CHEN Huanming; HU Benfu; LI Huiying; YU Quanmao; ZHANG Yiwen
School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083; School of Physics and Electrical Information Engineering; Ningxia University; Yinchuan 750021
Cite this article: 

CHEN Huanming; HU Benfu; LI Huiying; YU Quanmao; ZHANG Yiwen. Microstructure Characteristics of FGH95 Superalloy Powders Prepared by Prep. Acta Metall Sin, 2003, 39(1): 30-34 .

Download:  PDF(242KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  12 April 2002     
ZTFLH:  TF125.212  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/30

[1] Zhang Y, Li S K, Chen S D. Powder Metall Ind, 1998; 8(6) : 17(张莹,李世魁,陈生大.粉末冶金工业, 1998;8(6) :17)
[2] Hu B F, Zhang S H. J Univ Sci Technol Beijing, 1994;1(1) : 1
[3] He C Q, Hu B F, Guo W M, Chen S D. Ada Metall Sin,2000; 36: 187(何承群,胡本芙,国为民,陈生大.金属学报,2000;36:187)
[4] Gutierrez-miravete E, Lavernia E J, Trapaga G M,Szekely J, Grant N J. Metall Trans, 1989; 20A: 71
[5] Lee E-S, Ahn S. Ada Metall Mater, 1994; 42: 3231
[6] Liu Y Z, Chen Z H, Wang J N. Mater Sci Eng, 2000;A280: 229
[7] Grant P S, Cantor B, Katgerman L. Acta Metall Mater,1993; 41: 3079
[8] Cai W D, Lavernia E J. Metall Mater Trans, 1998; 29B:1085
[9] Sun J F, Shen J , Li Z Y, Jia J , Li Q C. Powder MetallTechnol, 2000; 18(2) : 92(孙剑飞,沈军,李振宇,贾军,李庆春.粉末冶金技术,2000;18(2) :92)
[10] Zhang J R, Zhao T Y. Handbook of Engineering Materials for Thermo-Physical Properties. Beijing: New Era Press, 1987(张家荣,赵廷元.工程常用物质的热物理性质手册.北京:新时代出版社,1987)
[11] Colin J. S Metals Reference Book, 5th ed. London & Boston: Butterworth & Co Ltd, 1976: 944
[12] Xu C W. Introduction to Calculation Methods. Beijing : High Education Press, 1985: 215(徐翠微.计算方法引论.北京:高等教育出版社,1985:215)]
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!