DYNAMIC AND THERMAL COMPUTATION OF Fe-66.7%Si DROPLETS FREE FALLING IN A DROP TUBE
WANG Haiyan; LIU Riping; ZHAN Zaiji; SUN Liling
Cite this article: 

WANG Haiyan; LIU Riping; ZHAN Zaiji; SUN Liling. DYNAMIC AND THERMAL COMPUTATION OF Fe-66.7%Si DROPLETS FREE FALLING IN A DROP TUBE. Acta Metall Sin, 2005, 41(9): 940-946 .

Download:  PDF(274KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The motion, microgravity level, and temperature of the Fe-66.7%Si (atomic fraction) droplets free falling in a drop tube filled with various inert gases under different pressures were computed. Based on the computation, the principle of choosing the proper inert gas and gas pressure was discussed in view of the gravity level and the melt cooling rate.
Key words:  Fe-66.7%Si droplet      drop tube      dynamic computation      
Received:  20 January 2005     
ZTFLH:  TG111  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I9/940

[1] Tani J, Kido H. J Appl Phys, 1999; 86: 464
[2] Leong D, Harry M, Reason K J, Homewood K P. Nature, 1997; 387: 686
[3] Kubaschewski O. Iron-Binary Phase Diagram. Berlin: Springer, 1982: 138
[4] Yamauchi I, Ueyama S, Ohnaka I. Mater Sci Eng, 1996; A208: 108
[5] Yamauchi I, Nagase T, Ohnaka I. J Alloy Compd, 1999; 292: 181
[6] Yamauchi I, Okamoto T, Ohata H, Ohnaka I. J Alloy Compd, 1997; 260: 162
[7] McCoy J K, Markworth A J, Brodkey R S, Collings E W. Mater Res Soc Symp Proc, 1987; 87: 163
[8] Evans N D, Hofmeister W H, Bayuzick R J, Robinson M B. Metall Trans, 1986; 17A: 973
[9] Lacy L L, Robinson M B, Evans N D, Bayuzick R J, Rathz T J. Mater Res Soc Symp Proc, 1982; 9: 87
[10] Pan M X, Chen X C. Physics, 1988; 17: 475 (潘明祥,陈熙琛.物理, 1988;17:475)
[11] Cliff R, Grace J R, Weber M E. Bubbles, Drops and Particles. New York: Academic Press, 1978: 111
[12] Brazhkin V V, Larchev V I, Popova S V, Skrotskaya G G. Phys Scr, 1989; 39: 338
[13] White F M. Viscous Fluid Flow. New York: McGrawHill, 1974: 35
[1] CHEN Liang; LUO Xinghong. A New Way to Explore Microgravity Effect by Drop Tube Experiment[J]. 金属学报, 2007, 43(7): 769-774 .
[2] WANG Nan; CAO Chongde; WEI Bingbo(Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072)Correspondent. WANG Nan; Doctoral candidate; Tel: (029)8493350; Fax: (029)8492074. RAPID SOLIDIFICATION OF Ag-Cu EUTECTIC ALLOY BY DROP TUBE PROCESSING[J]. 金属学报, 1998, 34(8): 824-830.
No Suggested Reading articles found!