Acta Metall Sin  2001, Vol. 37 Issue (1): 77-81     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2001, 37(1): 77-81 .

Download:  PDF(185KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  02 June 2000     
ZTFLH:  TG143.1  
  TG174.3  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2001/V37/I1/77

[1] Gahr K H Z, Eldis G T. Wear, 1980; 64: 175
[2] Parent S, Margerier J C. AFS Trans, 1972; 80: 393
[3] Gundlach R B. AFS Trans, 1974; 82; 309
[4] Dupin P, Saverna J, Schissler J M. AFS Trans,1982; 90:711
[5] Xing J D, Zhou Q D. AFS Trans, 1992; 100: 17
[6] Wu W Z, Xing J D, Su J Y. Acta Metall Sin, 1997; 33:1075(武文忠,邢建东,苏俊义.金属学报,1997;33:1075)
[7] Pitt C H, Chang Y M. Corrosion, 1986; 42: 312
[8] Bronson A, Nelson J, Kang C. Wear, 1992; 154: 387
[9] Zhou Q D. Chromium Anti-Wear Cast Iron. Xi'an: Xi'anJiaotong University Publishing House, 1987: 102(周庆德.铬系抗磨铸铁.西安:西安交通大学出版社,1987:102)
[10] Jiang X X, Wang J Y. Alloy Phase Electrochemistry.Shanghai: Shanghai Science and Technology PublishingHouse. 1984: 90(姜晓霞,王景蕴.合金相电化学.上海:上海科学技术出版社,1984:90)
[11] Xu J. Corrosion Metal and Resist Corrosion Metal Material. Hangzhou: Zhejiang Science and Technology Publishing House, 1981: 129(徐 坚.腐蚀金属学及耐腐蚀金属材料.杭州:浙江科学技术出版社,1981:129)
[12] Zhang A F, Xing J D, Gao Y M, Su J Y. Acta Metall Sin,2000; 36: 765(张安峰,邢建东,高义民,苏俊义.金属学报,2000;36:765)
[13] Zhang A F, Xing J D, Gao Y M, Su J Y. J Xi'an JiaotongUniv, 2000; 34(9): 88(张安峰,邢建东,高义民,苏俊义.西安交通大学学报,2000;34(9):88)
[14] Zheng Y G, Yao Z M, Wei X Y, Ke W. Wear, 1995; 186-187: 555`
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!