Please wait a minute...
Acta Metall Sin  2001, Vol. 37 Issue (1): 82-86     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2001, 37(1): 82-86 .

Download:  PDF(196KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  23 March 2000     
ZTFLH:  TG174.444  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2001/V37/I1/82

[1] Straede C A, Mikkelseen N J. Surf Coat Technol,1998;103/104: 189
[2] Wei R, Wilbur P J, Ozturk O. Nucl Instrum Methods,1991; B59/60:731
[3] Wilbur P J W, Buchholtz B. Surf Coat Technol,1996;79:1
[4] Wei R, Dhogrin B, Wilbur P J. J Tribol, 1994;. 116: 870
[5] Wei R, Wilbur P J, Sampath W S. J Tribol, 1991; 113:166
[6] Rehn L H, Aerback R S, Okamoto P R. Mater Sci Eng,1985; 69:1
[7] Terwagne G, Piette M, Bodart F. Mater Sci Eng, 1989;A115: 25
[8] Lueas S, Chevallier J, Chechen N G. Surf Coat Technol,1994; 66: 334
[9] Ohtani S, Inoue M, Takagi T. Nucl Instrum Methods,1997; B121: 319
[10] Vglov V V P, Rusalsky O P,. Vkhodasevich V. Surf CoatTechnol, 1998; 103/104: 323
[11] Zhang T H, Wu Y G. Optimizing Pressing of Ion Implantation. Beijing: Metallurgical industry Press, 1993: 155(张通和,吴瑜光.离子注入表面优化技术.北京:冶金工业出版社,1993:155)
[12] Zhang T H, Wu Y G, Ji C Z. Nucl Instrum Methods, 1992;B67: 458
[13] Wang A M, Ji C Z, Zhang T H. J Beijing Norm Univ(NatSci), 1992; 28: 482(王安明,姬成周,张通和.北京师范大学学报(自然科学版),1992;28:482)
[14] Ji C Z, Wang A M, Zhang T H. J Beijing Norm Univ (NatSci), 1992; 28: 323(姬成周,王安明,张通和.北京师范大学学报(自然科学版),1992;28:323)
[15] Ozturk O, Williamson D L. J Appl Phys, 1995; 77: 3839
[16] Zhang T H, Wu Y G. Material Modification Science andIts Application by Ion Beam. Beijing: Metallurgical Industry Press, 1999: 42(张通和,吴瑜光.离子束材料表面改性科学及应用.北京:冶金工业出版社,1999:42)
[17] Kpcewie M, Jagielski J, Gawlik G. Nucl Instram Methods,1995; B95: 208
[18] Bai B. Master Thesis, Southwest Jiaotong University,Chengdu, 1999: 47(白 彬.西南交通大学硕士学位论文,成都,1999:47)
[19] Shi D K. Dislocation and Strength of Materials. Xi'an:Xi'an Jiaotong University Press, 1988: 62(石德珂.位错与材料强度. 西安:西安交通大学出版社,1988:62)M
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!