Transformation Matrices for Determination of γ/γ Interface Types in Two-Phase TiAl Alloys |
CHEN Shanhua; G. Schumacher |
College of Materials and Bioengineering; Chengdu University of Technology; Chengdu 610059;Structure and Dynamics of Solids; Hahn--Meitner-Institut Berlin GmbH; 14109 Berlin; Germany |
|
Cite this article:
CHEN Shanhua; G. Schumacher. Transformation Matrices for Determination of γ/γ Interface Types in Two-Phase TiAl Alloys. Acta Metall Sin, 2004, 40(9): 903-908 .
|
Abstract The γ/γ lamellar interfaces play a critical role in the
mechanical properties of γ+α2
two-phase TiAl-based alloys. The transformation
matrices necessary for indexing the
crystallographical orientations of γ
lamella are systematically calculated. Based on these calculated
matrices, the interface types between neighboring γ
laths could be determined unambiguously.
The frequency of different interface types in a Ti-47Al-2Mn-2Nb
(atomic fraction, %)+0.8TiB2(volume fraction, %) alloy
was measured by means of convergent-beam electron
diffraction and compared with the frequency
distribution in binary TiAl alloys.
|
Received: 15 August 2003
|
|
[1] Chen Y Y, Kong P T. Acta Metall Sin, 2002; 38: 1141(陈玉勇,孔凡涛.金属学报,2002;38:1141) [2] Blackburn M J. In: Yaffe R, Promisel N, eds., The Science Technology and Applications of Titanium, Oxford: Pergamon, 1979: 633 [3] Inui H, Oh M H, Nakamura A, Yamaguchi M. Philos Mag,1992; 66A: 539 [4] Jin Z, Gray G T, Yamaguchi M. Philos Mag, 1998; 78A:239 [5] Zghal S, Naka S, Couret A. Acta Mater, 1997; 45: 3005 [6] Jin Z, Gray G T. Mater Sci Eng, 1997; A231: 62 [7] Yamaguchi M, Umakoshi Y. Prog Mater Sci, 1990; 34: 1 [8] Chen S H, Mukherji D, Schumacher G, Frohberg G, WahiR P. Mater Sci Eng, 2001; A300: 299 [9] Steeds J W. In: Hren J J, Goldstein J I, Joy D C, eds., Introduction to Analytical Electron Microscopy, New York: Plenum Press, 1979: 387 [10] Stadelmann P A. Ultramicroscopy, 1987; 21: 131 [11] Inui H, Nakamura A, Oh M H, Yamaguchi M. Philos Mag,1992; 66A: 557 [12] Inui H, Kishida K, Kobayashi M, Yamaguchi M, KawasakiM, Ibe K. Philos Mag, 1996; 74A: 451 [13] Denquin A, Naka S. Philos Mag Lett, 1993; 68: 13 |