Abstract The effect of constraint transformation heating temperature Th on the free reverse transformation behavior of 10\% strained
Ti44Ni47Nb9 alloy was investigated, and the
experimental results showed that after the first constraint transformation the strained Ti44Ni47Nb9 alloy exhibits two separate recovery strains εr1 and εr2 on subsequent free reverse transformation, which increases
and decreases with increasing Th, respectively. However, the total recovery strain εr(εr=εr1+εr2)of Ti44Ni47Nb9 alloy decreases with increasing Th. The plastic strain of Ti44Ni47Nb9 alloy is increased by the deformation of martensite under the recovery stress during the constraint
transformation, which decreases εr strain of
Ti44Ni47Nb9 alloy. Since the martensite
of strained Ti44Ni47Nb9 alloy
is consisted of M1 and M2 oriented martensites with different strain
levels after the first constraint transformation, strains εr1 and εr2
are related to M1 and M2 oriented martensite reverse transformations respectively.
|
|
Received: 16 April 2003
|
|
|
[1] Metlon K N, Simpson J, Duerig T W. Proc Int Conf on Martensitic Trans, 1986: 1053 [2] Melton K N, Proft J L, Duerig T W. Prog MRS Int Meeting on Advance Mater, 1988; 9: 165 [3] Zhao L C, Duerig T W, Justi S, Melton K N, Proft J L, Yu W, Wayman C M. Scr Metall Mater, 1990; 24: 221 [4] Cai W, Zhang C S, Zhao L C. J Mater Sci Technol, 1994; 10: 27 [5] Madagopal K, Ganesh R Krishnan, Banerjee S. Scr Metall, 1988; 22: 1593 [6] Brinson L C. J Intell Mater Syst Struct, 1993; 4: 229 [7] Wen Y H, Li N, Tu M J. Scr Mater, 2001; 44: 1113 [8] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater Trans JIM, 1993; 34: 919 [9] Lin H C, Wu S K. Ada Metall Mater, 1994; 42: 1623 [10] Liu X P, Jin W, Cao M Z, Yang D Z, Chen F X. Acta Metall Sin, 2002; 38: 193(刘晓鹏,金伟,曹名洲,杨大智,陈(?)(?).金属学报,2002;38:193) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|