| EFFECT OF EXTERNAL STRESS ON THE GROWTH OF PRECIPITATES IN Al--Cu AND Al--Cu--Mg--Ag ALLOYS |
|
Cite this article:
. EFFECT OF EXTERNAL STRESS ON THE GROWTH OF PRECIPITATES IN Al--Cu AND Al--Cu--Mg--Ag ALLOYS. Acta Metall Sin, 2004, 40(8): 799-804 .
|
|
|
|
|
Received: 01 January 1900
|
[1] Bogers A J. Acta Metali, 1962; 10: 260 [2] Hosford W F, Agrawal S P. Metali Trans, 1975; 6A: 4879 [3] Eto T, Sato A, Mori T. Acta Metali, 1978; 26: 499 [4] Tanaka Y, Sato A, Mori T. Acta Metali, 1978; 26: 529 [5] Skrotzki B, Shiflet G J, Starke E A Jr. Metall MaterTrans, 1996; 27A: 3431 [6] Zhu A W, Starke E A Jr. Acta Mater, 2001; 49: 2285 [7] Miyazaki T, Nakamura K, Mori H. J Mater Sci, 1979; 14:1827 [8] Nishizawa H, Sukedai E, Liu W, Hashimoto H. MaterTrans JIM, 1998; 39: 609 [9] Mukhopadhyay A K, Murken J, Skrotzki B, Eggeler G.Mater Sci Forum, 2000; 331-337: 1555 [10] Li D Y, Chen L Q. Acta Mater, 1998; 46: 2573 [11] Rossiter P L. The Electrical Resistivity of Metals and Alloys, London: Cambridge University Press, 1987: 107 [12] Hull S, Messoloras S, Stewart R J. Phil Mag A, 1988; 57:261 [13] Suh I S, Park J K. cer Metall Mater, 1995; 33: 205 [14] Reich L, Murayama M, Hono K. Acta Mater, 1998; 46: 6053 [15] Huchinson C R, Fan X, Pennycook S J, Shiflet G J. ActaMater, 2001; 49: 2827 [16] Ringer S P, Yeung W, Muddle B C, Polmear I J. ActaMetali Mater, 1994; 42: 1715 [17] Howe J M. Philos Mag Lett, 1994; 70: 111 [18] Fonda R W, Cassada W A, Shiflet G J. Acta Metali Mater,1992; 40: 2539 [19] Eshelby J D. Proc R Soc A, 1957; 241, 376 [20] Eshelby J D. Proc R Soc A, 1959; 252, 561 [21] Eshelby J D. Prog Solid Mech, 1961; 2, 87 [22] Mura T. Micromechanics of Defects in Solids, 2nd edition,Dordrech: Martinus Nijhoff, 1987: 177 [23] Fukikawa S, Hirano K. Defect and Diffusion Forum,Brandrain: Trans Tech Publications Ltd, 1989; 66-69: 447 [24] Dahmer U, Westmacott K H. Phys Status Solidi (a), 1983;80: 249 [25] Stobbs W M, Purdy G R. Acta Metall, 1978; 26: 1069 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|