| Density Measurement of Liquid Indium Using r--Ray Attenuation Method |
| WANG Lianwen; XIAN Aiping;SHAO Hanru |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
WANG Lianwen; XIAN Aiping; SHAO Hanru. Density Measurement of Liquid Indium Using r--Ray Attenuation Method. Acta Metall Sin, 2004, 40(6): 643-.
|
|
|
Abstract By means of r--ray attenuation method, the density of pure In and its relationship with temperature were measured in both solid and liquid states. The results show that the density data of pure In obtained by this method have a good repeatability within heating run and cooling run each other.
|
|
Received: 26 May 2003
|
|
|
[1] Iida T, Guthrie R I L. The Physical Properties of Liquid Metals. New York: Clarendon Press, 1988: 47 [2] Bian S M, Ma L M, Wang J T. Acta Metall Sin, 1986;22(2) : B90(边茂恕,马禄铭,王景唐.金属学报,1986;22(2) :B90) [3] Zhou G Z, Cai W J, Hu J H. J Univ Sci Technol Beijing,1991; 13(4. I): 380(周国治,蔡文娟,胡建虹、北京科技大学学报,1991;13(4. I):380) [4] Chen X M, Wang Q, Lu K Q. J Phys: Cond Matt, 1999;11: 10335 [5] Han X J, Wang N, Wei B. Philos Mag Lett, 2002; 82(8) :451 [6] Wang W M, Bian X F, Wang H R, Wang Z, Zhang L, Liu Z G. J Mater Res, 2001; 16: 3592 [7] Doge G. Z Naturforschg, 1966; 21a: 266 [8] Dillon I G, Levert F E, Loretan P A, Menon G U, Siddiqi F M, Tarng H J. Nucl Technol, 1973; 12: 307 [9] Basin A S, Kolotov Y L, Stankus S V. High Temp High Press, 1979; 11: 465 [10] Peggs I A. Thermal Expansion 6. New York: Plenum Press, 1978: 83 [11] Drotning W D. High Temp High Press, 1981; 13: 441 [12] Nasch P M, Steinemann S G. Phys Chem Liq, 1995; 29:43 [13] Smith P M, Elmer J W, Gallegos G F. Scr Mater, 1999;40(8) : 937 [14] Fudan University Tsinghua University Peking Universityed. Experimental Technique in Nuclear Physics (2nd ed).Beijing: Nuclear Energy Press, 1985: 81(复旦大学,清华大学,北京大学合编.原子核物理实验方法(第二版).北京:原子能出版社,1985:81) [15] Lide D R. CRC Handbook of Chemistry and Physics (78th ed). Chemical Rubber Company Press, 1998 [16] Williams D D, Miller R R. J Am Chem Soc, 1950; 72:3821 [17] Schneider A, Heymer G. Z Anorg Allg Chem, 1956; 286:97 [18] McGonigal P J, Cahill J A, Kirshenbaum A D. J Inorg Nucl Chem, 1962; 24: 1012 [19] Berthou P E, Tougas R. Metall Trans, 1970; 1: 2978 [20] Crawley A F. Trans AIME, 1968; 242: 2237 [21] McClelland M A, Sze J S. Surf Sci, 1995; 330(3) : 313 [22] Wang L W, Wang Q, Xian A P, Lu K Q. J Phys Cond Matt, 2003; 15: 777 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|