| Hydrogenation of Nitrobenzene Catalyzed by Pt Supported on Carbon Coated Nickel Magnetic Supports |
WU Yi1, SI Yang1, HUANG Yanmin2, DIAO Jiangyong1, MENG Fanjing2, LIU Zeng2, LIU Hongyang1( ) |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 Technology Innovation Center of Modified Isocyanate of Hebei Province, Cangzhou Dahua Co. Ltd., Cangzhou 061000, China |
|
Cite this article:
WU Yi, SI Yang, HUANG Yanmin, DIAO Jiangyong, MENG Fanjing, LIU Zeng, LIU Hongyang. Hydrogenation of Nitrobenzene Catalyzed by Pt Supported on Carbon Coated Nickel Magnetic Supports. Acta Metall Sin, 2024, 60(8): 1141-1149.
|
|
|
Abstract Aniline is an important chemical raw material widely used in various industries, including medicine, dye manufacturing, and rubber production. Catalytic liquid-phase dhydrogenation of nitrobenzene is a main industrial production method for aniline. However, the separation and recovery of the catalyst from the liquid hydrogenation system remain challenging. Graphene-encapsulated transition-metal nanoparticles (TM@G, where TM = Fe, Co, and Ni) exhibit magnetic separability and electron transfer effects, making them widely applicable in heterogeneous catalysis. In this study, a magnetically separable catalyst support, comprising graphene-encapsulated Ni nanoparticles (Ni@NG), was developed. This support was then loaded with a Pt metal catalyst for efficient catalytic hydrogenation of nitrobenzene to aniline. To fabricate the catalyst support, ethylenediaminetetraacetic acid and Ni(OH)2 were uniformly mixed in deionized water until the solution turned blue at 90°C. The resulting blue solid precursor was then dried and annealed at 600°C in argon to yield the magnetic support (Ni@NG). The support was then characterized using Raman spectroscopy, TEM, XRD, and XPS. TEM results revealed that the Ni@NG support exhibited a typical core-shell structure (with nanoscale Ni particles as the core and 2-5 layers of graphene as the shell). The Raman spectrum of the Ni@NG support exhibited the characteristic D and G bands of graphene at 1341 and 1604 cm-1, respectively. Moreover, the XRD spectrum of this support exhibited distinct peaks corresponding to Ni and graphene, while its XPS analysis confirmed the presence of an approximate nitrogen atom concentration of 3.64% in the nitrogen-doped graphene shell. Furthermore, the deposition-precipitation method was employed to synthesize a Pt-loaded Ni@NG catalyst (Pt/Ni@NG), which was later used in the catalytic hydrogenation of nitrobenzene in a liquid-phase reaction. Results revealed that increasing the Pt weight loading (mass fraction) from 0.1% to 0.5% altered the Pt dispersion state from single atoms to clusters and then to particles. In particular, at a Pt weight loading of 0.3%, the Pt/Ni@NG catalyst dominated by Pt clusters exhibited the highest activity for the hydrogenation of nitrobenzene. At this Pt weight loading, the catalyst achieved a turnover frequency of 27239.2 h-1 at 1 MPa reaction pressure under 30°C, completely converting nitrobenzene to aniline within 60 min. Furthermore, the Pt/Ni@NG catalyst maintained its activity over five testing cycles, attributed to its excellent liquid-phase magnetic separability.
|
|
Received: 11 March 2024
|
|
|
| Fund: National Natural Science Foundation of China(22072162);National Natural Science Foundation of China(U21B2092);Institutionalization Research Platform Project by Chinese Academy of Sciences, and Science and Technology Achievement Transfer Projec by Hebei Province and Chinese Academy of Sciences(23291401Z) |
Corresponding Authors:
LIU Hongyang, professor, Tel: (024)83970027, E-mail: liuhy@imr.ac.cn
|
| 1 |
Serna P, Corma A. Transforming nano metal nonselective particulates into chemoselective catalysts for hydrogenation of substituted nitrobenzenes [J]. ACS Catal., 2015, 5: 7114
|
| 2 |
Advani J H, Ravi K, Naikwadi D R, et al. Bio-waste chitosan-derived N-doped CNT-supported Ni nanoparticles for selective hydrogenation of nitroarenes [J]. Dalton Trans., 2020, 49: 10431
doi: 10.1039/d0dt01708f
pmid: 32676630
|
| 3 |
Meng X C, Cheng H Y, Akiyama Y, et al. Selective hydrogenation of nitrobenzene to aniline in dense phase carbon dioxide over Ni/γ-Al2O3: Significance of molecular interactions [J]. J. Catal., 2009, 264: 1
|
| 4 |
Li Z J, Zhang M Y, Dong X L, et al. Strong electronic interaction of indium oxide with palladium single atoms induced by quenching toward enhanced hydrogenation of nitrobenzene [J]. Appl. Catal., 2022, 313B: 121462
|
| 5 |
Yu H B, Liu J L, Wan Q Q, et al. Synergistic effect of acid-base and redox properties of nano Au/CeO2-cube on selective hydrogenation of nitrobenzene to aniline [J]. Mol. Catal., 2023, 540: 113045
|
| 6 |
Hajdu V, Prekob Á, Muránszky G, et al. Amine functionalization leads to enhanced performance for nickel- and cobalt-ferrite-supported palladium catalysts in nitrobenzene hydrogenation [J]. Int. J. Mol. Sci., 2023, 24: 13347
|
| 7 |
Polshettiwar V, Luque R, Fihri A, et al. Magnetically recoverable nanocatalysts [J]. Chem. Rev., 2011, 111: 3036
doi: 10.1021/cr100230z
pmid: 21401074
|
| 8 |
Chen M Q, Jiang X, Hu Q F, et al. Toehold-containing three-way junction-initiated multiple exponential amplification and CRISPR/Cas14a assistant magnetic separation enhanced visual detection of Mycobacterium tuberculosis [J]. ACS Sens., 2024, 9: 62
|
| 9 |
Lu D K, Qin M H, Liu C, et al. Ionic liquid-functionalized magnetic metal-organic framework nanocomposites for efficient extraction and sensitive detection of fluoroquinolone antibiotics in environmental water [J]. ACS Appl. Mater. Interfaces, 2021, 13: 5357
|
| 10 |
Zhang X X, Chen G P, Fu X, et al. Magneto-responsive microneedle robots for intestinal macromolecule delivery [J]. Adv. Mater., 2021, 33: 2104932
|
| 11 |
Zhang K, Ran J R, Zhu B C, et al. Nanoconfined nickel@carbon core-shell cocatalyst promoting highly efficient visible-light photocatalytic H2 production [J]. Small, 2018, 14: 1801705
|
| 12 |
Zhao L M, Qin X T, Zhang X R, et al. A magnetically separable Pd single-atom catalyst for efficient selective hydrogenation of phenylacetylene [J]. Adv. Mater., 2022, 34: 2110455
|
| 13 |
Wu J, Jin M, Li Y, et al. Earth-abundant Co nanoparticles encapsulated in N-doped hollow carbon sphere for highly selective hydrodeoxygenation of biomass-derived vanillin [J]. Chem. Eng. J., 2023, 463: 142472
|
| 14 |
Tu Y C, Deng J, Ma C, et al. Double-layer hybrid chainmail catalyst for high-performance hydrogen evolution [J]. Nano Energy, 2020, 72: 104700
|
| 15 |
Chang J F, Wang G Z, Chang X X, et al. Interface synergism and engineering of Pd/Co@N-C for direct ethanol fuel cells [J]. Nat. Commun., 2023, 14: 1346
doi: 10.1038/s41467-023-37011-z
pmid: 36906649
|
| 16 |
Meng X Y, Ma C, Jiang L Z, et al. Distance synergy of MoS2-confined rhodium atoms for highly efficient hydrogen evolution [J]. Angew. Chem. Int. Ed., 2020, 59: 10502
|
| 17 |
Deng D H, Yu L, Chen X Q, et al. Iron encapsulated within pod-like carbon nanotubes for oxygen reduction reaction [J]. Angew. Chem. Int. Ed., 2013, 52: 371
doi: 10.1002/anie.201204958
pmid: 23225769
|
| 18 |
Gao J, Ma R, Feng L, et al. Ambient hydrogenation and deuteration of alkenes using a nanostructured Ni-core-shell catalyst [J]. Angew. Chem., 2021, 133: 18739
|
| 19 |
Lv X W, Xu W S, Tian W W, et al. Activity promotion of core and shell in multifunctional core-shell Co2P@NC electrocatalyst by secondary metal doping for water electrolysis and Zn-air batteries [J]. Small, 2021, 17: 2101856
|
| 20 |
Li S, Yao N, Fan L L, et al. Supported Ni0@C-N catalyst with dual-reaction surfaces: Structure-performance relation in the selective hydrogenation of p-chloronitrobenzene [J]. Appl. Surf. Sci., 2022, 606: 154786
|
| 21 |
Du J, Lin Q Y, Zhang J Q, et al. N-doped core-shell mesoporous carbon spheres embedded by Ni nanoparticles for CO2 electroreduction [J]. Rare Met., 2023, 42: 2284
|
| 22 |
Cerezo-Navarrete C, Marin I M, García-Miquel H, et al. Magnetically induced catalytic reduction of biomass-derived oxygenated compounds in water [J]. ACS Catal., 2022, 12: 8462
doi: 10.1021/acscatal.2c01696
pmid: 37528952
|
| 23 |
Kuo C T, Lu Y B, Kovarik L, et al. Structure sensitivity of acetylene semi-hydrogenation on Pt single atoms and subnanometer clusters [J]. ACS Catal., 2019, 9: 11030
|
| 24 |
Gu R T, Meng D M, She M Y, et al. Appropriate aggregation is needed for highly active Pt/Al2O3 to enable hydrogenation of chlorinated nitrobenzene [J]. Chem. Commun., 2022, 58: 7630
|
| 25 |
Wang H H, Shi F X, Pu M, et al. Theoretical study on nitrobenzene hydrogenation by N-doped carbon-supported late transition metal single-atom catalysts [J]. ACS Catal., 2022, 12: 11518
|
| 26 |
Zhang Q S, Bu J H, Wang J D, et al. Highly efficient hydrogenation of nitrobenzene to aniline over Pt/CeO2 catalysts: The shape effect of the support and key role of additional Ce3+ sites [J]. ACS Catal., 2020, 10: 10350
|
| 27 |
Liu L C, Concepción P, Corma A. Modulating the catalytic behavior of non-noble metal nanoparticles by inter-particle interaction for chemoselective hydrogenation of nitroarenes into corresponding azoxy or azo compounds [J]. J. Catal., 2019, 369: 312
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|