Hydrogenation of Nitrobenzene Catalyzed by Pt Supported on Carbon Coated Nickel Magnetic Supports
WU Yi1, SI Yang1, HUANG Yanmin2, DIAO Jiangyong1, MENG Fanjing2, LIU Zeng2, LIU Hongyang1()
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 Technology Innovation Center of Modified Isocyanate of Hebei Province, Cangzhou Dahua Co. Ltd., Cangzhou 061000, China
Cite this article:
WU Yi, SI Yang, HUANG Yanmin, DIAO Jiangyong, MENG Fanjing, LIU Zeng, LIU Hongyang. Hydrogenation of Nitrobenzene Catalyzed by Pt Supported on Carbon Coated Nickel Magnetic Supports. Acta Metall Sin, 2024, 60(8): 1141-1149.
Aniline is an important chemical raw material widely used in various industries, including medicine, dye manufacturing, and rubber production. Catalytic liquid-phase dhydrogenation of nitrobenzene is a main industrial production method for aniline. However, the separation and recovery of the catalyst from the liquid hydrogenation system remain challenging. Graphene-encapsulated transition-metal nanoparticles (TM@G, where TM = Fe, Co, and Ni) exhibit magnetic separability and electron transfer effects, making them widely applicable in heterogeneous catalysis. In this study, a magnetically separable catalyst support, comprising graphene-encapsulated Ni nanoparticles (Ni@NG), was developed. This support was then loaded with a Pt metal catalyst for efficient catalytic hydrogenation of nitrobenzene to aniline. To fabricate the catalyst support, ethylenediaminetetraacetic acid and Ni(OH)2 were uniformly mixed in deionized water until the solution turned blue at 90°C. The resulting blue solid precursor was then dried and annealed at 600°C in argon to yield the magnetic support (Ni@NG). The support was then characterized using Raman spectroscopy, TEM, XRD, and XPS. TEM results revealed that the Ni@NG support exhibited a typical core-shell structure (with nanoscale Ni particles as the core and 2-5 layers of graphene as the shell). The Raman spectrum of the Ni@NG support exhibited the characteristic D and G bands of graphene at 1341 and 1604 cm-1, respectively. Moreover, the XRD spectrum of this support exhibited distinct peaks corresponding to Ni and graphene, while its XPS analysis confirmed the presence of an approximate nitrogen atom concentration of 3.64% in the nitrogen-doped graphene shell. Furthermore, the deposition-precipitation method was employed to synthesize a Pt-loaded Ni@NG catalyst (Pt/Ni@NG), which was later used in the catalytic hydrogenation of nitrobenzene in a liquid-phase reaction. Results revealed that increasing the Pt weight loading (mass fraction) from 0.1% to 0.5% altered the Pt dispersion state from single atoms to clusters and then to particles. In particular, at a Pt weight loading of 0.3%, the Pt/Ni@NG catalyst dominated by Pt clusters exhibited the highest activity for the hydrogenation of nitrobenzene. At this Pt weight loading, the catalyst achieved a turnover frequency of 27239.2 h-1 at 1 MPa reaction pressure under 30°C, completely converting nitrobenzene to aniline within 60 min. Furthermore, the Pt/Ni@NG catalyst maintained its activity over five testing cycles, attributed to its excellent liquid-phase magnetic separability.
Fund: National Natural Science Foundation of China(22072162);National Natural Science Foundation of China(U21B2092);Institutionalization Research Platform Project by Chinese Academy of Sciences, and Science and Technology Achievement Transfer Projec by Hebei Province and Chinese Academy of Sciences(23291401Z)
Corresponding Authors:
LIU Hongyang, professor, Tel: (024)83970027, E-mail: liuhy@imr.ac.cn
Fig.1 HRTEM images of Ni@NG support with different magnifications (a-d), high angle annular dark field (HAADF) STEM image of Ni@NG support (e), and size distributions of Ni nanoparticles in Ni@NG support (f) (Inset in Fig.1d shows the selected area electron diffraction pattern, d—lattice spacing)
Fig.2 XPS results of the Ni@NG support (a) N1s (b) C1s (c) Ni2p (d) O1s
Fig.3 Raman spectrum (a) and thermogravimetric (TG) curves (b) of the as-prepared Ni@NG support (ID / IG—intensity ratio)
Fig.4 Schematics of the Ni@NG support with magnetic separability under the hydrogenation system (a) the as-prepared Ni@NG sample was dispersed into the solvent (b) then a magnet is placed on one side for 1 min
Fig.5 Low (a, c, e) and high (b, d, f) magnified HAADF STEM images of 0.1%Pt1/Ni@NG (a, b), 0.3%Ptn/Ni@NG (c, d), and 0.5%Ptp/Ni@NG (e, f) catalysts (White labels indicate Pt single atoms, blue labels indicate Pt nanoparticles, and red labels indicate Pt clusters)
Fig.6 XRD spectra of Ni@NG support and 0.1%Pt1/Ni@NG, 0.3%Ptn/Ni@NG, and 0.5%Ptp/Ni@NG catalysts
Fig.7 N2 adsorption/desorption isotherms (a, b) and pore size distribution curves (c, d) of Ni@NG support (a, c) and 0.3%Ptn/Ni@NG catalyst (b, d) (Vads—N2 adsorption volume, D—pore size)
Fig.8 Turnover frequency (TOF) for 0.1%Pt1/Ni@NG, 0.3%Ptn/Ni@NG, and 0.5%Ptp/Ni@NG catalysts (a); nitrobenzene hydrogenation kinetic curves (b), time-nitrobenzene conversion rates and aniline yield curve (c), and hydrogenation stability (d) of 0.3%Ptn/Ni@NG catalyst (T—absolute temperature; r—reaction rate constant at temperature T; Ea—experimental activation energy)
1
Serna P, Corma A. Transforming nano metal nonselective particulates into chemoselective catalysts for hydrogenation of substituted nitrobenzenes [J]. ACS Catal., 2015, 5: 7114
2
Advani J H, Ravi K, Naikwadi D R, et al. Bio-waste chitosan-derived N-doped CNT-supported Ni nanoparticles for selective hydrogenation of nitroarenes [J]. Dalton Trans., 2020, 49: 10431
doi: 10.1039/d0dt01708f
pmid: 32676630
3
Meng X C, Cheng H Y, Akiyama Y, et al. Selective hydrogenation of nitrobenzene to aniline in dense phase carbon dioxide over Ni/γ-Al2O3: Significance of molecular interactions [J]. J. Catal., 2009, 264: 1
4
Li Z J, Zhang M Y, Dong X L, et al. Strong electronic interaction of indium oxide with palladium single atoms induced by quenching toward enhanced hydrogenation of nitrobenzene [J]. Appl. Catal., 2022, 313B: 121462
5
Yu H B, Liu J L, Wan Q Q, et al. Synergistic effect of acid-base and redox properties of nano Au/CeO2-cube on selective hydrogenation of nitrobenzene to aniline [J]. Mol. Catal., 2023, 540: 113045
6
Hajdu V, Prekob Á, Muránszky G, et al. Amine functionalization leads to enhanced performance for nickel- and cobalt-ferrite-supported palladium catalysts in nitrobenzene hydrogenation [J]. Int. J. Mol. Sci., 2023, 24: 13347
Chen M Q, Jiang X, Hu Q F, et al. Toehold-containing three-way junction-initiated multiple exponential amplification and CRISPR/Cas14a assistant magnetic separation enhanced visual detection of Mycobacterium tuberculosis [J]. ACS Sens., 2024, 9: 62
9
Lu D K, Qin M H, Liu C, et al. Ionic liquid-functionalized magnetic metal-organic framework nanocomposites for efficient extraction and sensitive detection of fluoroquinolone antibiotics in environmental water [J]. ACS Appl. Mater. Interfaces, 2021, 13: 5357
10
Zhang X X, Chen G P, Fu X, et al. Magneto-responsive microneedle robots for intestinal macromolecule delivery [J]. Adv. Mater., 2021, 33: 2104932
11
Zhang K, Ran J R, Zhu B C, et al. Nanoconfined nickel@carbon core-shell cocatalyst promoting highly efficient visible-light photocatalytic H2 production [J]. Small, 2018, 14: 1801705
12
Zhao L M, Qin X T, Zhang X R, et al. A magnetically separable Pd single-atom catalyst for efficient selective hydrogenation of phenylacetylene [J]. Adv. Mater., 2022, 34: 2110455
13
Wu J, Jin M, Li Y, et al. Earth-abundant Co nanoparticles encapsulated in N-doped hollow carbon sphere for highly selective hydrodeoxygenation of biomass-derived vanillin [J]. Chem. Eng. J., 2023, 463: 142472
14
Tu Y C, Deng J, Ma C, et al. Double-layer hybrid chainmail catalyst for high-performance hydrogen evolution [J]. Nano Energy, 2020, 72: 104700
15
Chang J F, Wang G Z, Chang X X, et al. Interface synergism and engineering of Pd/Co@N-C for direct ethanol fuel cells [J]. Nat. Commun., 2023, 14: 1346
doi: 10.1038/s41467-023-37011-z
pmid: 36906649
16
Meng X Y, Ma C, Jiang L Z, et al. Distance synergy of MoS2-confined rhodium atoms for highly efficient hydrogen evolution [J]. Angew. Chem. Int. Ed., 2020, 59: 10502
17
Deng D H, Yu L, Chen X Q, et al. Iron encapsulated within pod-like carbon nanotubes for oxygen reduction reaction [J]. Angew. Chem. Int. Ed., 2013, 52: 371
doi: 10.1002/anie.201204958
pmid: 23225769
18
Gao J, Ma R, Feng L, et al. Ambient hydrogenation and deuteration of alkenes using a nanostructured Ni-core-shell catalyst [J]. Angew. Chem., 2021, 133: 18739
19
Lv X W, Xu W S, Tian W W, et al. Activity promotion of core and shell in multifunctional core-shell Co2P@NC electrocatalyst by secondary metal doping for water electrolysis and Zn-air batteries [J]. Small, 2021, 17: 2101856
20
Li S, Yao N, Fan L L, et al. Supported Ni0@C-N catalyst with dual-reaction surfaces: Structure-performance relation in the selective hydrogenation of p-chloronitrobenzene [J]. Appl. Surf. Sci., 2022, 606: 154786
21
Du J, Lin Q Y, Zhang J Q, et al. N-doped core-shell mesoporous carbon spheres embedded by Ni nanoparticles for CO2 electroreduction [J]. Rare Met., 2023, 42: 2284
22
Cerezo-Navarrete C, Marin I M, García-Miquel H, et al. Magnetically induced catalytic reduction of biomass-derived oxygenated compounds in water [J]. ACS Catal., 2022, 12: 8462
doi: 10.1021/acscatal.2c01696
pmid: 37528952
23
Kuo C T, Lu Y B, Kovarik L, et al. Structure sensitivity of acetylene semi-hydrogenation on Pt single atoms and subnanometer clusters [J]. ACS Catal., 2019, 9: 11030
24
Gu R T, Meng D M, She M Y, et al. Appropriate aggregation is needed for highly active Pt/Al2O3 to enable hydrogenation of chlorinated nitrobenzene [J]. Chem. Commun., 2022, 58: 7630
25
Wang H H, Shi F X, Pu M, et al. Theoretical study on nitrobenzene hydrogenation by N-doped carbon-supported late transition metal single-atom catalysts [J]. ACS Catal., 2022, 12: 11518
26
Zhang Q S, Bu J H, Wang J D, et al. Highly efficient hydrogenation of nitrobenzene to aniline over Pt/CeO2 catalysts: The shape effect of the support and key role of additional Ce3+ sites [J]. ACS Catal., 2020, 10: 10350
27
Liu L C, Concepción P, Corma A. Modulating the catalytic behavior of non-noble metal nanoparticles by inter-particle interaction for chemoselective hydrogenation of nitroarenes into corresponding azoxy or azo compounds [J]. J. Catal., 2019, 369: 312