| Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature |
BAI Juju1,2, LI Jianjian1,2( ), FU Chonglong1,2, CHEN Shuangjian1, LI Zhijun1, LIN Jun1,2( ) |
1Shanghai Institute of Applied Physics, Chinese Academy of Sciences, Shanghai 201800, China 2University of Chinese Academy of Sciences, Beijing 100049, China |
|
Cite this article:
BAI Juju, LI Jianjian, FU Chonglong, CHEN Shuangjian, LI Zhijun, LIN Jun. Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature. Acta Metall Sin, 2024, 60(3): 299-310.
|
|
|
Abstract GH3535 high-temperature nickel-based alloy was selected as the main structural material for the molten salt reactor because of its high-temperature strength and excellent corrosion resistance to molten salts. In general, the welded joints used to join structural materials are considered as the potentially weakest part because of the inhomogeneity in microstructure caused by repeated thermal cycle treatments. Helium embrittlement at high temperatures is an important issue that affects the safety and structural integrity of the components made of nickel-based alloys working in a reactor environment. In this study, the GH3535-welded joint was irradiated with 500 keV of He ions at 850oC. The microstructure and mechanical properties of the weld and base metal were characterized and compared by TEM and nano-indentation, and the effect of the intrinsic microstructure of the weld on the irradiation effect was investigated. Results show that the helium bubbles in the weld are basically distributed on the dislocation lines and carbide-base metal interface. The helium bubbles on the carbides-base metal interface are smaller, and they have higher density than those on the dislocation lines. The average number density of helium bubbles and dislocation loops in the peak damage region of the weld are smaller than those of the base metal. Therefore, at 850oC, dislocation lines, and the carbides-base metal interface are strong traps for helium and interstitial atoms, which affect the nucleation of helium bubbles and dislocation loops. In addition, the carbides-base metal interface can effectively inhibit the growth of helium bubbles. The results of nano-indentation show that the degree of the irradiation-induced hardening of the weld metal (36%) is about half of that of the base metal (70%) under the same irradiation condition. Therefore, the DBH model confirms that helium bubbles and dislocation loops primarily cause irradiation hardening. The enhanced trapping of helium atoms and interstitials by nano-carbides and dislocation lines at a high temperature is the key factor for the distinct irradiation behavior of welds compared with base metals.
|
|
Received: 27 January 2022
|
|
|
| Fund: National Natural Science Foundation of China(12175301);National Natural Science Foundation of China(11605272);Frontier Science Key Program of Chinese Academy of Sciences(QYZDY-SSW-JSC016);Strategic Priority Research Program of Chinese Academy of Sciences(XDA02030200);Natural Science Foundation of Shanghai(22ZR1474800);Heavy Ion Research Facility in Lanzhou (HIRFL)(HIR2021PY007) |
Corresponding Authors:
LI Jianjian, professor, Tel: (021)39194239, E-mail: lijianjian@sinap.ac.cn; LIN Jun, professor, Tel: (021)39194026, E-mail: linjun@sinap.ac.cn
|
| 1 |
Yvon P, Carré F. Structural materials challenges for advanced reactor systems [J]. J. Nucl. Mater., 2009, 385: 217
doi: 10.1016/j.jnucmat.2008.11.026
|
| 2 |
Chen S J, Tsang D K L, Jiang L, et al. Microstructure and local strains in GH3535 alloy heat affected zone and their influence on the mechanical properties [J]. Mater. Sci. Eng., 2017, A699: 48
|
| 3 |
Chen S J, Ye X X, Yu K, et al. Microstructure and mechanical properties of UNS N10003 alloy welded joints [J]. Mater. Sci. Eng., 2017, A682: 168
|
| 4 |
Huang H F, Zhou X L, Li C W, et al. Temperature dependence of nickel ion irradiation damage in GH3535 alloy weld metal [J]. J. Nucl. Mater., 2017, 497: 108
doi: 10.1016/j.jnucmat.2017.06.005
|
| 5 |
Li F G, Lei Y C, Zhang X N, et al. Study on microstructure change and hardening of 316L steel weld seam after helium ion irradiation [J]. Fusion Eng. Des., 2019, 148: 111293
doi: 10.1016/j.fusengdes.2019.111293
|
| 6 |
Was G S. Fundamentals of Radiation Materials Science [M]. Berlin: Springer, 2007: 827
|
| 7 |
Zinkle S J, Busby J T. Structural materials for fission & fusion energy [J]. Mater. Today, 2009, 12: 12
|
| 8 |
Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735
doi: 10.1016/j.actamat.2012.11.004
|
| 9 |
McCoy H E. An evaluation of the molten-salt reactor experiment Hastelloy N surveillance speciments—Fourth group [R]. Oak Ridge: Oak Ridge National Laboratory, 1971
|
| 10 |
Fu C L, Li J J, Bai J J, et al. Effect of helium bubbles on irradiation hardening of additive manufacturing 316L stainless steel under high temperature He ions irradiation [J]. J. Nucl. Mater., 2021, 550: 152948
doi: 10.1016/j.jnucmat.2021.152948
|
| 11 |
Zhu Z B, Huang H F, Muránsky O, et al. On the irradiation tolerance of nano-grained Ni-Mo-Cr alloy: 1 MeV He+ irradiation experiment [J]. J. Nucl. Mater., 2021, 544: 152694
doi: 10.1016/j.jnucmat.2020.152694
|
| 12 |
Gao J, Huang H F, Liu J Z, et al. Coalescence mechanism of helium bubble during tensile deformation revealed by in situ small-angle X-ray scattering [J]. Scr. Mater., 2019, 158: 121
doi: 10.1016/j.scriptamat.2018.08.050
|
| 13 |
Bai J J, Li J J, Fu C L, et al. Temperature dependence of He bubble evolution in UNS N10003 alloys under He ion irradiation [J]. J. Appl. Phys., 2021, 130: 155901
doi: 10.1063/5.0064975
|
| 14 |
Trinkaus H, Singh B N. Helium accumulation in metals during irradiation-where do we stand? [J]. J. Nucl. Mater., 2003, 323: 229
doi: 10.1016/j.jnucmat.2003.09.001
|
| 15 |
Zhang C H, Chen K Q, Wang Y S, et al. Formation of bubbles in helium implanted 316L stainless steel at temperatures between 25 and 550oC [J]. J. Nucl. Mater., 1997, 245: 210
doi: 10.1016/S0022-3115(97)00007-X
|
| 16 |
Kesternich W. Helium trapping at dislocations, precipitates and grain boundaries [J]. Radiat. Eff., 1983, 78: 261
doi: 10.1080/00337578308207376
|
| 17 |
Lin Y R, Chen W Y, Tan L Z, et al. Bubble formation in helium-implanted nanostructured ferritic alloys at elevated temperatures [J]. Acta Mater., 2021, 217: 117165
doi: 10.1016/j.actamat.2021.117165
|
| 18 |
Edmondson P D, Parish C M, Zhang Y, et al. Helium entrapment in a nanostructured ferritic alloy [J]. Scr. Mater., 2011, 65: 731
doi: 10.1016/j.scriptamat.2011.07.024
|
| 19 |
Li C, Lei G H, Liu J Z, et al. A potential candidate structural material for molten salt reactor: ODS nickel-based alloy [J]. J. Mater. Sci. Technol., 2022, 109: 129
doi: 10.1016/j.jmst.2021.08.071
|
| 20 |
Bai J J, Li J J, Fu C L, et al. Effect of helium bubbles on the irradiation hardening of GH3535 welded joints at 650oC [J]. J. Nucl. Mater., 2021, 557: 153241
doi: 10.1016/j.jnucmat.2021.153241
|
| 21 |
Chen Q, Zhang K, Liu R D, et al. Irradiation damage in GH3535 alloy under He ion irradiation at high temperature [J]. At. Energy Sci. Technol., 2020, 54: 688
|
|
陈 倩, 张 柯, 刘仁多 等. 高温He离子辐照GH3535合金的损伤效应 [J]. 原子能科学技术, 2020, 54: 688
|
| 22 |
Ziegler J F, Biersack J P. The stopping and range of ions in matter [A]. Treatise on Heavy-Ion Science [M]. New York: Springer, 1985: 93
|
| 23 |
ASTM. Standard practice for neutron radiation damage simulation by charged-particle irradiation [S]. West Conshohocken: ASTM International, 2009
|
| 24 |
Jiang L, Song M, Yang L Q, et al. A comparison study of void swelling in additively manufactured and cold-worked 316L stainless steels under ion irradiation [J]. J. Nucl. Mater., 2021, 551: 152946
doi: 10.1016/j.jnucmat.2021.152946
|
| 25 |
Edwards D J, Simonen E P, Bruemmer S M. Evolution of fine-scale defects in stainless steels neutron-irradiated at 275oC [J]. J. Nucl. Mater., 2003, 317: 13
doi: 10.1016/S0022-3115(03)00002-3
|
| 26 |
Nix W D, Gao H J. Indentation size effects in crystalline materials: A law for strain gradient plasticity [J]. J. Mech. Phys. Solids, 1998, 46: 411
doi: 10.1016/S0022-5096(97)00086-0
|
| 27 |
Kasada R, Takayama Y, Yabuuchi K, et al. A new approach to evaluate irradiation hardening of ion-irradiated ferritic alloys by nano-indentation techniques [J]. Fusion Eng. Des., 2011, 86: 2658
doi: 10.1016/j.fusengdes.2011.03.073
|
| 28 |
Ding J H, Sun D, Yang Y C, et al. First-principles investigations of intrinsic point defects and helium impurities in vanadium monocarbide [J]. Nucl. Instrum. Methods Phys. Res., 2020, 479B: 163
|
| 29 |
Wright R N, Van Siclen C D. In-situ TEM observations of helium bubble interactions with dislocations [J]. J. Nucl. Mater., 1993, 206: 87
doi: 10.1016/0022-3115(93)90237-S
|
| 30 |
Li Y P, Ran G, Guo Y J, et al. The evolution of dislocation loop and its interaction with pre-existing dislocation in He+-irradiated molybdenum: In-situ TEM observation and molecular dynamics simulation [J]. Acta Mater., 2020, 201: 462
doi: 10.1016/j.actamat.2020.10.022
|
| 31 |
Liu P P, Zhao M Z, Zhu Y M, et al. Effects of carbide precipitate on the mechanical properties and irradiation behavior of the low activation martensitic steel [J]. J. Alloys Compd., 2013, 579: 599
doi: 10.1016/j.jallcom.2013.07.085
|
| 32 |
Lucas G E. The evolution of mechanical property change in irradiated austenitic stainless steels [J]. J. Nucl. Mater., 1993, 206: 287
doi: 10.1016/0022-3115(93)90129-M
|
| 33 |
Foreman A J E, Makin M J. Dislocation movement through random arrays of obstacles [J]. Can. J. Phys., 1967, 45: 511
doi: 10.1139/p67-044
|
| 34 |
Gan J, Was G S. Microstructure evolution in austenitic Fe-Cr-Ni alloys irradiated with rotons: Comparison with neutron-irradiated microstructures [J]. J. Nucl. Mater., 2001, 297: 161
doi: 10.1016/S0022-3115(01)00615-8
|
| 35 |
Katoh Y, Ando M, Kohyama A. Radiation and helium effects on microstructures, nano-indentation properties and deformation behavior in ferrous alloys [J]. J. Nucl. Mater., 2003, 323: 251
doi: 10.1016/j.jnucmat.2003.08.007
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|