|
|
|
| Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine |
DU Zonggang( ), XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng |
| Xi'an Aerospace Propulsion Test Technique Institute, Xi'an 710100, China |
|
Cite this article:
DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine. Acta Metall Sin, 2023, 59(10): 1335-1345.
|
|
|
Abstract Hydrogen is clean energy that can replace traditional fossil fuels in the future because of its high energy density, easy recharging, and availability of current liquid fuel infrastructure. However, the polymer-electrolyte membrane fuel cell requires controlled storage and efficient hydrogen release. Recently, liquid-phase chemical hydrogen storage materials with high gravimetric hydrogen density have emerged as promising candidates to overcome such challenges. Among these materials of interest, hydrous hydrazine (N2H4·H2O) is the best candidate; however, it has not been fully explored as an alternative for chemical hydrogen storage applications. A catalyst is essential to hydrogen production at a sufficient reaction rate for N2H4·H2O-based hydrogen generation systems. In this study, a series of supported Ni100 - x Ir x /Al2O3 catalysts were prepared using simple impregnation, roasting, and reduction method. The effect of reaction conditions on the activity and selectivity was evaluated in decomposing N2H4·H2O to hydrogen. The phase/structure of the catalysts was characterized using XRD, TEM, XPS, BET, and H2-TPD to gain insight into the catalytic performance of the Ni100 - x Ir x /Al2O3 catalysts. It indicated that the Ni60Ir40/Al2O3 catalyst, comprising Ni-Ir alloy nanoparticles with an average size of 2-4 nm and crystalline γ-Al2O3, exhibited excellent catalytic activity (> 200 h-1) and selectivity (> 99%) toward hydrogen generation from N2H4·H2O at different temperatures, from 293 K to 353 K. The Ni60Ir40/Al2O3 catalyst is durable and stable; however, the catalytic activity decreased from 249.2 to 225.0 h-1 (~9.7%) after five runs with 99% H2 selectivity at 323 K toward the dehydrogenation of N2H4·H2O. In addition, parameters, such as temperature, N2H4·H2O and NaOH concentration, and catalyst mass on N2H4·H2O decomposition were investigated over the Ni60Ir40/Al2O3 catalyst. The kinetic rate equation for catalytic decomposition of N2H4·H2O could be represented using the following expression: r = -k[N2H4·H2O]0.346/0.054[NaOH]0.307[Catalyst]1.004, where k = 4.62 × 109exp(-5088.49 / T). The results could provide a theoretical foundation for applying N2H4·H2O as a promising hydrogen storage material.
|
|
Received: 15 August 2021
|
|
|
| Fund: Special Fund of Shaanxi Key Laboratory of Special Fuel Chemistry and Material(SPCF-SKL-2020-0006) |
Corresponding Authors:
DU Zonggang, professor, Tel: (029)85602796, E-mail: 165s8yf@163.com
|
| 1 |
Jang Y B, Kim T H, Sun M H, et al. Preparation of iridium catalyst and its catalytic activity over hydrazine hydrate decomposition for hydrogen production and storage [J]. Catal. Today, 2009, 146: 196
doi: 10.1016/j.cattod.2009.01.040
|
| 2 |
Lang C G, Jia Y, Yao X D. Recent advances in liquid-phase chemical hydrogen storage [J]. Energy Stor. Mater., 2020, 26: 290
|
| 3 |
Jofre J B F, Soares Neto T G, Dias F F, et al. Evaluation of Ir/Al2O3, Ir-Ru/Al2O3 and Ru/Al2O3 catalyst performance in a 5 N satellite thruster [J]. Acta Astron., 2013, 85: 41
doi: 10.1016/j.actaastro.2012.12.008
|
| 4 |
Prasad V, Vasanthkumar M S. Iridium-decorated multiwall carbon nanotubes and its catalytic activity with Shell 405 in hydrazine decomposition [J]. J. Nanopart. Res., 2015, 17: 398
doi: 10.1007/s11051-015-3199-7
|
| 5 |
Kang W, Guo H, Varma A. Noble-metal-free NiCu/CeO2 catalysts for H2 generation from hydrous hydrazine [J]. Appl. Catal., 2019, 249B: 54
|
| 6 |
Zou H T, Guo F, Luo M H, et al. La(OH)3-decorated NiFe nanoparticles as efficient catalyst for hydrogen evolution from hydrous hydrazine and hydrazine borane [J]. Int. J. Hydrogen Energy, 2020, 45: 11641
doi: 10.1016/j.ijhydene.2020.02.074
|
| 7 |
Tong D G. Retraction: Mesoporous multiwalled carbon nanotubes as supports for monodispersed iron-boron catalysts: Improved hydrogen generation from hydrous hydrazine decomposition [J]. J. Mater. Chem., 2020, 8A: 6908
|
| 8 |
He L, Huang Y Q, Liu X Y, et al. Structural and catalytic properties of supported Ni-Ir alloy catalysts for H2 generation via hydrous hydrazine decomposition [J]. Appl. Catal., 2014, 147B: 779
|
| 9 |
Zhong Y J, Dai H B, Zhu M, et al. Catalytic decomposition of hydrous hydrazine over Ni-Pt/La2O3 catalyst: A high-performance hydrogen storage system [J]. Int. J. Hydrogen Energy, 2016, 41: 11042
doi: 10.1016/j.ijhydene.2016.03.207
|
| 10 |
Chen Y, Wang L, Zhai Y N, et al. Pd-Ni nanoparticles supported on reduced graphene oxides as catalysts for hydrogen generation from hydrazine [J]. RSC Adv., 2017, 7: 32310
doi: 10.1039/C7RA04390B
|
| 11 |
Qiu Y P, Yin H, Dai H, et al. Tuning the surface composition of Ni/meso-CeO2 with iridium as an efficient catalyst for hydrogen generation from hydrous hydrazine [J]. Chem. Eur. J., 2018, 24: 4902
doi: 10.1002/chem.v24.19
|
| 12 |
Gao Y, Wang Q, He T, et al. Defective crystalline molybdenum phosphides as bifunctional catalysts for hydrogen evolution and hydrazine oxidation reactions during water splitting [J]. Inorg. Chem. Front., 2019, 6: 2686
doi: 10.1039/C9QI01005J
|
| 13 |
Hong X L, Yao Q L, Huang M L, et al. Bimetallic NiIr nanoparticles supported on lanthanum oxy-carbonate as highly efficient catalysts for hydrogen evolution from hydrazine borane and hydrazine [J]. Inorg. Chem. Front., 2019, 6: 2271
doi: 10.1039/C9QI00848A
|
| 14 |
Firdous N, Janjua N K, Qazi I, et al. Optimal Co-Ir bimetallic catalysts supported on γ-Al2O3 for hydrogen generation from hydrous hydrazine [J]. Int. J. Hydrogen Energy, 2016, 41: 984
doi: 10.1016/j.ijhydene.2015.10.084
|
| 15 |
Zhao P P, Cao N, Su J, et al. NiIr nanoparticles immobilized on the pores of MIL-101 as highly efficient catalyst toward hydrogen generation from hydrous hydrazine [J]. ACS Sustain. Chem. Eng., 2015, 3: 1086
doi: 10.1021/acssuschemeng.5b00009
|
| 16 |
Shi Q, Qiu Y P, Dai H, et al. Study of formation mechanism of Ni-Pt/CeO2 catalyst for hydrogen generation from hydrous hydrazine [J]. J. Alloys Compd., 2019, 787: 1187
doi: 10.1016/j.jallcom.2019.01.378
|
| 17 |
Zhao P P, Cao N, Luo W, et al. Nanoscale MIL-101 supported RhNi nanoparticles: An efficient catalyst for hydrogen generation from hydrous hydrazine [J]. J. Mater. Chem., 2015, 3A: 12468
|
| 18 |
Xu L X, Liu N, Hong B, et al. Nickel-platinum nanoparticles immobilized on graphitic carbon nitride as highly efficient catalyst for hydrogen release from hydrous hydrazine [J]. RSC Adv., 2016, 6: 31687
doi: 10.1039/C6RA01335J
|
| 19 |
Wang W, Hong X L, Yao Q L, et al. Bimetallic Ni-Pt nanoparticles immobilized on mesoporous N-doped carbon as a highly efficient catalyst for complete hydrogen evolution from hydrazine borane [J]. J. Mater. Chem., 2020, 8A: 13694
|
| 20 |
Karatas Y, Gülcan M, Zahmakiran M. Silica supported ternary NiRuPt alloy nanoparticles: Highly efficient heterogeneous catalyst for H2 generation via selective decomposition of hydrous hydrazine in alkaline solution [J]. Int. J. Hydrogen Energy, 2020, 45: 27098
doi: 10.1016/j.ijhydene.2020.07.048
|
| 21 |
Qiu Y P, Dai H, Dai H B, et al. Tuning surface composition of Ni-Pt/CeO2 catalyst for hydrogen generation from hydrous hydrazine decomposition [J]. Acta Metall. Sin., 2018, 54: 1289
|
|
丘玉萍, 戴 豪, 戴洪斌 等. 适于水合肼分解制氢的Ni-Pt/CeO2催化剂的表面组分调控 [J]. 金属学报, 2018, 54: 1289
doi: 10.11900/0412.1961.2017.00481
|
| 22 |
Chen J M, Zou H T, Yao Q L, et al. Cr2O3-modified NiFe nanoparticles as a noble-metal-free catalyst for complete dehydrogenation of hydrazine in aqueous solution [J]. Appl. Surf. Sci., 2020, 501: 144247
doi: 10.1016/j.apsusc.2019.144247
|
| 23 |
Dai H B, Zhong Y J, Wang P. Hydrogen generation from decomposition of hydrous hydrazine over Ni-Ir/CeO2 catalyst [J]. Prog. Nat. Sci.: Mater. Int., 2017, 27: 121
doi: 10.1016/j.pnsc.2016.12.012
|
| 24 |
Wang Y T, Pan L, Chen Y X, et al. Mo-doped Ni-based catalyst for remarkably enhancing catalytic hydrogen evolution of hydrogen-storage materials [J]. Int. J. Hydrogen Energy, 2020, 45: 15560
doi: 10.1016/j.ijhydene.2020.04.061
|
| 25 |
Dai H, Dai H B, Zhong Y J, et al. Kinetics of catalytic decomposition of hydrous hydrazine over CeO2-supported bimetallic Ni-Pt nanocatalysts [J]. Int. J. Hydrogen Energy, 2017, 42: 5684
doi: 10.1016/j.ijhydene.2016.10.160
|
| 26 |
Soares Neto T G, Cobo A J G, Cruz G M. Evolution of morphologic properties on the preparation of Ir/Al2O3 catalysts with high metallic contents [J]. Appl. Surf. Sci., 2005, 240: 355
doi: 10.1016/j.apsusc.2004.07.002
|
| 27 |
Zhang J S, Delgass W N, Fisher T S, et al. Kinetics of Ru-catalyzed sodium borohydride hydrolysis [J]. J. Power Sources, 2007, 164: 772
doi: 10.1016/j.jpowsour.2006.11.002
|
| 28 |
Zhong Y J, Dai H B, Wang P. Preparation of Ni-Pt/La2O3 catalyst and its kinetics study of hydrous hydrazine for hydrogen generation [J]. Acta Metall. Sin., 2016, 52: 505
|
|
钟玉洁, 戴洪斌, 王 平. 水合肼制氢Ni-Pt/La2O3催化剂研制及其反应动力学研究 [J]. 金属学报, 2016, 52: 505
doi: 10.11900/0412.1961.2015.00531
|
| 29 |
Al-Thubaiti K S, Khan Z. Trimetallic nanocatalysts to enhanced hydrogen production from hydrous hydrazine: The role of metal centers [J]. Int. J. Hydrogen Energy, 2020, 45: 13960
doi: 10.1016/j.ijhydene.2020.03.093
|
| 30 |
Motta D, Barlocco I, Bellomi S, et al. Hydrous hydrazine decomposition for hydrogen production using of Ir/CeO2: Effect of reaction parameters on the activity [J]. Nanomaterials, 2021, 11: 1340
doi: 10.3390/nano11051340
|
| 31 |
Contour J P, Pannetier G. Hydrazine decomposition over a supported iridium catalyst [J]. J. Catal., 1972, 24: 434
doi: 10.1016/0021-9517(72)90127-3
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|