Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine
DU Zonggang(), XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng
Xi'an Aerospace Propulsion Test Technique Institute, Xi'an 710100, China
Cite this article:
DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine. Acta Metall Sin, 2023, 59(10): 1335-1345.
Hydrogen is clean energy that can replace traditional fossil fuels in the future because of its high energy density, easy recharging, and availability of current liquid fuel infrastructure. However, the polymer-electrolyte membrane fuel cell requires controlled storage and efficient hydrogen release. Recently, liquid-phase chemical hydrogen storage materials with high gravimetric hydrogen density have emerged as promising candidates to overcome such challenges. Among these materials of interest, hydrous hydrazine (N2H4·H2O) is the best candidate; however, it has not been fully explored as an alternative for chemical hydrogen storage applications. A catalyst is essential to hydrogen production at a sufficient reaction rate for N2H4·H2O-based hydrogen generation systems. In this study, a series of supported Ni100 - x Ir x /Al2O3 catalysts were prepared using simple impregnation, roasting, and reduction method. The effect of reaction conditions on the activity and selectivity was evaluated in decomposing N2H4·H2O to hydrogen. The phase/structure of the catalysts was characterized using XRD, TEM, XPS, BET, and H2-TPD to gain insight into the catalytic performance of the Ni100 - x Ir x /Al2O3 catalysts. It indicated that the Ni60Ir40/Al2O3 catalyst, comprising Ni-Ir alloy nanoparticles with an average size of 2-4 nm and crystalline γ-Al2O3, exhibited excellent catalytic activity (> 200 h-1) and selectivity (> 99%) toward hydrogen generation from N2H4·H2O at different temperatures, from 293 K to 353 K. The Ni60Ir40/Al2O3 catalyst is durable and stable; however, the catalytic activity decreased from 249.2 to 225.0 h-1 (~9.7%) after five runs with 99% H2 selectivity at 323 K toward the dehydrogenation of N2H4·H2O. In addition, parameters, such as temperature, N2H4·H2O and NaOH concentration, and catalyst mass on N2H4·H2O decomposition were investigated over the Ni60Ir40/Al2O3 catalyst. The kinetic rate equation for catalytic decomposition of N2H4·H2O could be represented using the following expression: r = -k[N2H4·H2O]0.346/0.054[NaOH]0.307[Catalyst]1.004, where k = 4.62 × 109exp(-5088.49 / T). The results could provide a theoretical foundation for applying N2H4·H2O as a promising hydrogen storage material.
Fig.1 TEM images of Ni100 - x Ir x /Al2O3 catalysts samples (d—diameter of particle) (a) Ni/Al2O3 (b) Ni80lr20/Al2O3 (c) Ni60lr40/Al2O3 (d) Ni40lr60/Al2O3 (e) Ni20lr80/Al2O3 (f) lr/Al2O3
Fig.2 XRD spectra of Ni100 - x Ir x /Al2O3 catalysts samples
Fig.3 XPS results of Ni100 - x Ir x /Al2O3 catalysts (a) Ni2p (b) Ir4f (c) O1s
Fig.4 N2 adsorption/desorption isotherm curves of Al2O3 carrier and Ni60Ir40/Al2O3 catalyst (STP—standard temperature and pressure, P is the partial pressure of nitrogen, and P0 is the saturated vapor pressure of nitrogen at liquid nitrogen temperature)
Sample
Specific surface area / (cm2·g-1)
Pore volume / (mL·g-1)
Pore diameter / nm
Al2O3
195.25
0.33
5.3
Ni60Ir40/Al2O3
171.83
0.28
4.8
Table 1 Comparisons of BET resutts between Al2O3 carrier and Ni60Ir40/Al2O3 catalyst
Fig.5 Time course profiles for the N2H4·H2O decomposition over the Ni100 - x Ir x /Al2O3 catalysts (a) and effect of Ir content (molar ratio) in the catalyst on the reaction rate (r) and H2 selectivity (b) ( / —molar fraction of (H2 + N2) to N2H4)
Catalyst sample
H2 selectivity / %
r / h-1
Ni/Al2O3
88.38
2.8
NiIr0.1/Al2O3
> 99
10.7
Ni99Ir1/Al2O3
> 99
47.4
Ni90Ir10/Al2O3
> 99
109.8
Ni80Ir20/Al2O3
> 99
125.0
Ni60Ir40/Al2O3
> 99
249.2
Ni40Ir60/Al2O3
96.25
321.4
Ni20Ir80/Al2O3
21.03
642.9
Ir/Al2O3
8.58
725.8
Table 2 Comparisons of catalytic performance of the Ni100 - x Ir x /Al2O3 catalysts
Fig.6 Effects of reaction temperature on N2H4·H2O decomposition in the presence of Ni60Ir40/Al2O3 (a) and NiIr0.1/Al2O3 (c), and the responding reaction rates for the activation energy determination according Arrhenius equation (R2—goodness of fit) (b, d)
Fig.7 Time profiles for the total gas volume () from the catalytic decomposition of N2H4·H2O solutions with varied concentrations (a), effects of N2H4·H2O concentration on its initial reaction rate in the presence of Ni60Ir40/Al2O3 at 303 K (b), and plots of lnrvs ln[N2H4·H2O] with low (c) and high (d) N2H4·H2O concentrations
Fig.8 Effects of NaOH concentration on N2H4·H2O decomposition in the presence of Ni60Ir40/Al2O3 (a) and a plot of lnr vs ln[NaOH] (b)
Fig.9 Effects of catalyst concentration on N2H4·H2O decomposition in the presence of Ni60Ir40/Al2O3 (a) and a plot of vs ln[catalyst] (b)
Fig.10 Durability test for H2 generation from N2H4·H2O over Ni60Ir40/Al2O3 catalyst (a) and the H2-TPD profiles of fresh and post-used catalysts (b) (TPD—temperature programmed desorption)
1
Jang Y B, Kim T H, Sun M H, et al. Preparation of iridium catalyst and its catalytic activity over hydrazine hydrate decomposition for hydrogen production and storage [J]. Catal. Today, 2009, 146: 196
doi: 10.1016/j.cattod.2009.01.040
2
Lang C G, Jia Y, Yao X D. Recent advances in liquid-phase chemical hydrogen storage [J]. Energy Stor. Mater., 2020, 26: 290
3
Jofre J B F, Soares Neto T G, Dias F F, et al. Evaluation of Ir/Al2O3, Ir-Ru/Al2O3 and Ru/Al2O3 catalyst performance in a 5 N satellite thruster [J]. Acta Astron., 2013, 85: 41
doi: 10.1016/j.actaastro.2012.12.008
4
Prasad V, Vasanthkumar M S. Iridium-decorated multiwall carbon nanotubes and its catalytic activity with Shell 405 in hydrazine decomposition [J]. J. Nanopart. Res., 2015, 17: 398
doi: 10.1007/s11051-015-3199-7
5
Kang W, Guo H, Varma A. Noble-metal-free NiCu/CeO2 catalysts for H2 generation from hydrous hydrazine [J]. Appl. Catal., 2019, 249B: 54
6
Zou H T, Guo F, Luo M H, et al. La(OH)3-decorated NiFe nanoparticles as efficient catalyst for hydrogen evolution from hydrous hydrazine and hydrazine borane [J]. Int. J. Hydrogen Energy, 2020, 45: 11641
doi: 10.1016/j.ijhydene.2020.02.074
7
Tong D G. Retraction: Mesoporous multiwalled carbon nanotubes as supports for monodispersed iron-boron catalysts: Improved hydrogen generation from hydrous hydrazine decomposition [J]. J. Mater. Chem., 2020, 8A: 6908
8
He L, Huang Y Q, Liu X Y, et al. Structural and catalytic properties of supported Ni-Ir alloy catalysts for H2 generation via hydrous hydrazine decomposition [J]. Appl. Catal., 2014, 147B: 779
9
Zhong Y J, Dai H B, Zhu M, et al. Catalytic decomposition of hydrous hydrazine over Ni-Pt/La2O3 catalyst: A high-performance hydrogen storage system [J]. Int. J. Hydrogen Energy, 2016, 41: 11042
doi: 10.1016/j.ijhydene.2016.03.207
10
Chen Y, Wang L, Zhai Y N, et al. Pd-Ni nanoparticles supported on reduced graphene oxides as catalysts for hydrogen generation from hydrazine [J]. RSC Adv., 2017, 7: 32310
doi: 10.1039/C7RA04390B
11
Qiu Y P, Yin H, Dai H, et al. Tuning the surface composition of Ni/meso-CeO2 with iridium as an efficient catalyst for hydrogen generation from hydrous hydrazine [J]. Chem. Eur. J., 2018, 24: 4902
doi: 10.1002/chem.v24.19
12
Gao Y, Wang Q, He T, et al. Defective crystalline molybdenum phosphides as bifunctional catalysts for hydrogen evolution and hydrazine oxidation reactions during water splitting [J]. Inorg. Chem. Front., 2019, 6: 2686
doi: 10.1039/C9QI01005J
13
Hong X L, Yao Q L, Huang M L, et al. Bimetallic NiIr nanoparticles supported on lanthanum oxy-carbonate as highly efficient catalysts for hydrogen evolution from hydrazine borane and hydrazine [J]. Inorg. Chem. Front., 2019, 6: 2271
doi: 10.1039/C9QI00848A
14
Firdous N, Janjua N K, Qazi I, et al. Optimal Co-Ir bimetallic catalysts supported on γ-Al2O3 for hydrogen generation from hydrous hydrazine [J]. Int. J. Hydrogen Energy, 2016, 41: 984
doi: 10.1016/j.ijhydene.2015.10.084
15
Zhao P P, Cao N, Su J, et al. NiIr nanoparticles immobilized on the pores of MIL-101 as highly efficient catalyst toward hydrogen generation from hydrous hydrazine [J]. ACS Sustain. Chem. Eng., 2015, 3: 1086
doi: 10.1021/acssuschemeng.5b00009
16
Shi Q, Qiu Y P, Dai H, et al. Study of formation mechanism of Ni-Pt/CeO2 catalyst for hydrogen generation from hydrous hydrazine [J]. J. Alloys Compd., 2019, 787: 1187
doi: 10.1016/j.jallcom.2019.01.378
17
Zhao P P, Cao N, Luo W, et al. Nanoscale MIL-101 supported RhNi nanoparticles: An efficient catalyst for hydrogen generation from hydrous hydrazine [J]. J. Mater. Chem., 2015, 3A: 12468
18
Xu L X, Liu N, Hong B, et al. Nickel-platinum nanoparticles immobilized on graphitic carbon nitride as highly efficient catalyst for hydrogen release from hydrous hydrazine [J]. RSC Adv., 2016, 6: 31687
doi: 10.1039/C6RA01335J
19
Wang W, Hong X L, Yao Q L, et al. Bimetallic Ni-Pt nanoparticles immobilized on mesoporous N-doped carbon as a highly efficient catalyst for complete hydrogen evolution from hydrazine borane [J]. J. Mater. Chem., 2020, 8A: 13694
20
Karatas Y, Gülcan M, Zahmakiran M. Silica supported ternary NiRuPt alloy nanoparticles: Highly efficient heterogeneous catalyst for H2 generation via selective decomposition of hydrous hydrazine in alkaline solution [J]. Int. J. Hydrogen Energy, 2020, 45: 27098
doi: 10.1016/j.ijhydene.2020.07.048
21
Qiu Y P, Dai H, Dai H B, et al. Tuning surface composition of Ni-Pt/CeO2 catalyst for hydrogen generation from hydrous hydrazine decomposition [J]. Acta Metall. Sin., 2018, 54: 1289
Chen J M, Zou H T, Yao Q L, et al. Cr2O3-modified NiFe nanoparticles as a noble-metal-free catalyst for complete dehydrogenation of hydrazine in aqueous solution [J]. Appl. Surf. Sci., 2020, 501: 144247
doi: 10.1016/j.apsusc.2019.144247
23
Dai H B, Zhong Y J, Wang P. Hydrogen generation from decomposition of hydrous hydrazine over Ni-Ir/CeO2 catalyst [J]. Prog. Nat. Sci.: Mater. Int., 2017, 27: 121
doi: 10.1016/j.pnsc.2016.12.012
24
Wang Y T, Pan L, Chen Y X, et al. Mo-doped Ni-based catalyst for remarkably enhancing catalytic hydrogen evolution of hydrogen-storage materials [J]. Int. J. Hydrogen Energy, 2020, 45: 15560
doi: 10.1016/j.ijhydene.2020.04.061
25
Dai H, Dai H B, Zhong Y J, et al. Kinetics of catalytic decomposition of hydrous hydrazine over CeO2-supported bimetallic Ni-Pt nanocatalysts [J]. Int. J. Hydrogen Energy, 2017, 42: 5684
doi: 10.1016/j.ijhydene.2016.10.160
26
Soares Neto T G, Cobo A J G, Cruz G M. Evolution of morphologic properties on the preparation of Ir/Al2O3 catalysts with high metallic contents [J]. Appl. Surf. Sci., 2005, 240: 355
doi: 10.1016/j.apsusc.2004.07.002
27
Zhang J S, Delgass W N, Fisher T S, et al. Kinetics of Ru-catalyzed sodium borohydride hydrolysis [J]. J. Power Sources, 2007, 164: 772
doi: 10.1016/j.jpowsour.2006.11.002
28
Zhong Y J, Dai H B, Wang P. Preparation of Ni-Pt/La2O3 catalyst and its kinetics study of hydrous hydrazine for hydrogen generation [J]. Acta Metall. Sin., 2016, 52: 505
Al-Thubaiti K S, Khan Z. Trimetallic nanocatalysts to enhanced hydrogen production from hydrous hydrazine: The role of metal centers [J]. Int. J. Hydrogen Energy, 2020, 45: 13960
doi: 10.1016/j.ijhydene.2020.03.093
30
Motta D, Barlocco I, Bellomi S, et al. Hydrous hydrazine decomposition for hydrogen production using of Ir/CeO2: Effect of reaction parameters on the activity [J]. Nanomaterials, 2021, 11: 1340
doi: 10.3390/nano11051340
31
Contour J P, Pannetier G. Hydrazine decomposition over a supported iridium catalyst [J]. J. Catal., 1972, 24: 434
doi: 10.1016/0021-9517(72)90127-3
SUN Li; SONG Qihong; HU Zhuangqi (State Key Laboratory of Rapidly Solidified Nonequilibrium Alloy; Institute of Metal Research; Chinese Academy of Sciences; Shengyang 110015)(Manuscript received 1995-05-10; in revised form 1995-09-05). STRUCTURE AND CATALYTIC PROPERTIES OF RAPIDLY SOLIDIFIED Cu_(30)Al_(70)ALLOY[J]. 金属学报, 1996, 32(1): 63-68.
[7]
SUN Li; SONG Qihong; HU Zhuangqi(Stale Key Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-03-03; in revised form 1995-O5-05). FORMATION AND CATALYTIC ACTIVITY OF NANOCRYSTALLINE Cu_(30)Al_(70) ALLOY CATALYST[J]. 金属学报, 1995, 31(20): 341-345.