| MICROSTRUCTURE AND ROOM TEMPERATURE COMPRESSION PROPERTIES OF Mg82.13Zn13.85Y4.02 ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE |
DONG Yun1, LIN Xiaoping1( ), XU Rui2, FAN Zhibin1, YE Jie1, WANG Zhe2 |
1 Department of Materials Science and Engineering, Northeastern University, Shenyang 110819 2 State Key Laboratory of Metastable Materials Science and Technology, School of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 |
|
Cite this article:
DONG Yun, LIN Xiaoping, XU Rui, FAN Zhibin, YE Jie, WANG Zhe. MICROSTRUCTURE AND ROOM TEMPERATURE COMPRESSION PROPERTIES OF Mg82.13Zn13.85Y4.02 ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE. Acta Metall Sin, 2014, 50(5): 594-600.
|
|
|
Abstract By the investigation of the microstructures of Mg82.13Zn13.85Y4.02 (mass fraction, %) alloy solidified under different pressure, it is found that the solidification microstructure of the alloy is consisted of a-Mg matrix, W-Mg3Y2Zn3 phase and I-Mg3YZn6 phase. In the microstructure of the alloy solidified under ambient pressure, the networks of the secondary phases of eutectic-like and rod-like shape are distributed in the a-Mg interdendritic space. As the solidification pressure increases, eutectic network is disconnected gradually and the amount of eutectic is diminished and the solubility of Zn in a-Mg rises gradually. The results of the measurement of the mechanical properties show that the compression strength, the yield strength and the compressibility of the alloy sample solidified under ambient pressure is 344 MPa, 331 MPa and 16% respectively. However, the compression strength, the yield strength and the compressibility of the alloy sample solidified from 1250 ℃ under 6 GPa is 455 MPa, 426 MPa and 25%, respectively. The observation of fracture surfaces shows that, in the alloy solidified under high pressure, the cleavage surface of the compressed fracture is decreased, and the tear ridge and tearing dimple can be found. The degree of cleavage fracture is decreased.
|
|
Received: 21 August 2013
|
|
|
| Fund: Natural Science Foundation of Hebei Province (No.E2013501096), Natural Science Foundation of Liaoning Province (No.20112063) and Projiect of Science and Technology of Northeastern University at Qinhuangdao (No.XNK201305) |
| [1] |
Somekawa H, Watanabe H, Mukai T. Mater Lett, 2011; 65: 3251
|
| [2] |
Xu S W, Zheng M Y, Kamado S, Wu K, Wang G J, Lv X Y. Mater Sci Eng, 2011; A528: 4055
|
| [3] |
Luo S Q, Tang A T, Pan F S, Song K, Wang W Q. Trans Nonferrous Met Soc China, 2011; 21: 795
|
| [4] |
Chen B, Chen L, Lin D L, Zeng X Q. Trans Nonferrous Met Soc China, 2012; 22: 773
|
| [5] |
Wang J F, Gao S, Song P F, Huang X F, Shi Z Z, Pan F S. J Alloys Compd, 2011; 509: 8567
|
| [6] |
Yang W P, Guo X F, Lu Z X. Trans Nonferrous Met Soc China, 2012; 22: 786
|
| [7] |
Lee J Y, Kim D H, Lim H K, Kim D H. Mater Lett, 2005; 59: 3801
|
| [8] |
Tong J, Huang H, Yuan G Y, Ding W J. Acta Metall Sin, 2011; 47:1520
|
|
(童 健, 黄 华, 袁广银,丁文江. 金属学报, 2011; 47: 1520)
|
| [9] |
Somekawa H, Singh A, Mukai T. Adv Eng Mater, 2009; 11: 782
|
| [10] |
Luo Z P, Zhang S Q, Tang Y L, Zhao D S. Scr Metall Mater, 1993; 28: 1513
|
| [11] |
Tsai A, Niikura A, Inoue A. J Mater Res, 1997; 12: 565
|
| [12] |
Батншeв А И,translated byZhang J S. Crystallization of Metal and Alloys Under Pressure. Harbin: Harbin University of Techonology Press, 1987: 23
|
|
(Батншeв А И 著,张锦升 译. 金属和合金在压力下结晶. 哈尔滨: 哈尔滨工业大学出版社, 1987: 23)
|
| [13] |
Qu Y D, Li R D, Yuan X G, Li C X, Xiang Q C. Foundry, 2005; 54: 539
|
|
(曲迎东, 李荣德, 袁晓光, 李晨曦, 向青春. 铸造, 2005; 54: 539)
|
| [14] |
Zhang G Z, Yu X F, Wang X Y, Jia G L, Gao Y Y. Acta Metall Sin, 1999; 35: 285
|
|
(张国志, 于溪凤, 王向阳, 贾光霖, 高允彦. 金属学报, 1999; 35: 285)
|
| [15] |
Jie J C, Zou C M, Wang H W, Wei Z J. J Alloys Compd, 2010; 506: L12
|
| [16] |
Chen Y, Liu L, Wang Y H, Liu J H, Zhang R J. Trans Nonferrous Met Soc China, 2011; 21: 2205
|
| [17] |
Wang Z X, Lu J B, Xi Y J, Fan J W. J Alloys Compd, 2010; 492: 529
|
| [18] |
Wang D Q, Yang G C, Lin L, Feng Z G. Mater Lett, 2008; 62: 1711
|
| [19] |
Wang Z L, Zhang T, Li L, Zhou Y B, Wang H W, Wei Z J. Chin J Nonferrous Met, 2012; 22: 1006
|
|
(王振玲, 张 涛, 李 莉, 周月波, 王宏伟, 魏尊杰. 中国有色金属学报, 2012; 22: 1006)
|
| [20] |
Sun S H,Li J,Xu R,Zhao H L,Liu R P. Chin J High Pressure Phys, 2008; 22: 434
|
|
(孙淑华, 李 杰, 徐 瑞, 赵海丽, 刘日平. 高压物理学报, 2008; 22: 434)
|
| [21] |
Lin X P, Dong Y, Xu R, Sun G F, Jiao S H. Acta Metall Sin, 2011; 47: 1550
|
|
(林小娉, 董 允, 徐 瑞, 孙桂芳, 焦世辉. 金属学报, 2011; 47: 1550)
|
| [22] |
Lin X P, Dong Y, Xu R, Zheng R G. Rare Met Mater Eng, 2013; 42: 2309
|
|
(林小娉, 董 允, 徐 瑞, 郑润国. 稀有金属材料与工程, 2013; 42: 2309 )
|
| [23] |
Li B, Wang H W, Jie J C, Wei Z J. J Alloys Compd, 2011; 509: 3387
|
| [24] |
Ding W J. The Science and Technology of Mg Alloy. Beijing: Science Press, 2007: 1
|
|
(丁文江. 镁合金科学与技术. 北京: 科学出版社, 2007: 1)
|
| [25] |
Jiang X S,Zhao H. Quick Reference for Microscopic Fracture of Steel. Beijing: Machinery Industry Press, 2010: 45
|
|
(姜锡山,赵 晗. 钢铁显微断口速查手册. 北京: 机械工业出版社, 2010: 45)
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|