					Cite this article:
						|  |  
    					|  |  
    					| MICROSMICROSTRUCTURE AND MECHANICAL PROPERTIES OF SIMULATE FUSION LINE IN EH40 SHIP PLATE STEEL FOR HIGH HEAT INPUT WELDING |  
						| ZHANG Pengyan, GAO Cairu, ZHU Fuxian |  
						| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |  
						|  |  
					
			      ZHANG Pengyan GAO Cairu ZHU Fuxian. MICROSMICROSTRUCTURE AND MECHANICAL PROPERTIES OF SIMULATE FUSION LINE IN EH40 SHIP PLATE STEEL FOR HIGH HEAT INPUT WELDING. Acta Metall Sin, 2012, 48(3): 264-270.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  The microstructure and mechanical properties in simulate fusion line of EH40 ship plate steel with high heat inputs were investigated using welding thermal simulation test. The effects of inclusions on the grain size of original austenite and intragranular ferrite (IGF) were analyzed. The results indicate that impact energy of the steels at -20 ℃ was more than 150 J with a heat input of 800 kJ/cm (t8/5=730 s) and maximum temperature of 1400 ℃ for 30 s. The microstructures of the steel were composed of GBF, IPF and IAF, and the fraction of IAF was over 50%. Lath bainite and granular bainite were not observed. The type and concentration of inclusions were ideal which decreased the growth of GBF. Those inclusions whose diameter were 5-8 μm can also promote the formation of IGF, and sometimes IAF was also formed through the nucleation at Mn-depleted zone. |  
															| Received:  10 August 2011 |  
															| Fund: Supported by National Natural Science Foundation of China and Shanghai Baosteel (No.50834010), High Technology Research and Development Program of China (No.2009AA032530), Key Project of Chinese Ministry of Education (No.108036) |  
            
									            
									               
																												  
															| [1] Zhang H Q, Jiang L Z. Baosteel Technol, 2006; 4: 20(张汉谦, 江来珠. 宝钢技术, 2006; 4: 20)[2] Mi G S, Chen D Z, Qu F. Pet Chem Constr, 2009; 29(5): 25(米广生, 陈德志, 瞿 帆. 石油化工建设, 2009; 29(5): 25)[3] Luo X B, Su H, Yang C F, Chai F, Yuan X M. Trans China Weld Inst, 2010; 31(10): 57(罗小兵, 苏航, 杨才福, 柴锋, 袁晓敏. 焊接学报, 2010; 31(10): 57)[4] Suzuki S, Ichimiya K, Akita T. JFE Tech Rep, 2004; 5: 19[5] Hitoshi H. Tetsu Hagane, 2004; 5: 271[6] Minagawa M, Ishikawa T, Mabuchi H. CAMP–ISIJ, 1997; 10: 590[7] Hong S G, Kang K J, Park C G. Scr Mater, 2002; 6: 163[8] Vega M I, Medina S F, Quispe A, Gomez M, Gomez P P. ISIJ Int, 2005; 45: 1878[9] Kasamatsu Y. Tetsu Hagane, 1979; 65: 1232[10] Kojima A, Kiyose A, Minagawa M, Hirano A, Yoshii K, Nakajima T, Hoshino M, Ueshima Y. CAMP–ISIJ, 2003; 16: 360[11] Kiyomichi N, Akihiro Y, Sengo K, Masahiko H, Yuichi K. Tetsu Hagane, 2004; 90: 141[12] Qiu P J, Michihiko N. Tetsu Hagane, 1998; 84: 592[13] Matsuda S, Okumura N, Okamura Y. Tetsu Hagane, 1974; 60: 174[14] Matsuda S, Okumura N. Tetsu Hagane, 1976; 62: 1209[15] Kasamatsu Y, Takashima S, Hosoya T. Tetsu Hagane, 1976; 62: 678[16] Mukae S, Nishio K, Katoh M, Isayama T. PJWS, 1985; 3(3): 131[17] Koda M, Amano K, Funahashi Y, Shiga C, Ueda S. Tetsu Hagane, 1984; 70: 1265[18] ShuW, Wang X M, Li S R, He X L. Acta Metall Sin, 2011; 47: 435(舒玮, 王学敏, 李书瑞, 贺信莱. 金属学报, 2011; 47: 435)[19] Han S C. Dev Appl Mater, 1995; 10: 2[20] Murakani T, Takeda H, Nanba S. PJWS, 2004; 75: 324[21] Kang Y B, Lee H G. ISIJ Int, 2010; 50: 501[22] Yamamoto K, Jinichi T. ISIJ, 1996; 36: 80[23] Shim J, Cho Y. Acta Mater, 1999; 47: 2751[24] Ishikawa F, Takahashi F. ISIJ, 1995; 35: 1128[25] Madariaga I, Gutierrez I. Acta Mater, 1999; 47: 95[26] Enomoto M. Met Mater Int, 1998; 4: 115[27] Lee J L. Acta Metall Mater, 1994; 42: 3291[28] Pan Y T, Lee J L. Mater Des, 1994; 15: 331[29] Hong S G, Kang K J, Park C G. Scr Mater, 2002; 6: 163[30] Yamamoto K, Hasegawa T, Takamura J. ISIJ, 1996; 36: 80[31] Jinichi T, Shozo M. Proceedings of the Sixth Internal Iron and Steel Congress. Nagoya: Iron and Steel Institute of Japan, 1999: 591 |  
             
								                
															
																| 
																																																																									