| ON THE CONCENTRATION OF CADMIUM AND RECOVERY OF LEAD FROM THE LEAD BLAST FURNACE DUST |
| CHAO PEI-YING;LEE KENG-SHENG;FANG BING;TAN KWO YONG;WANG CHUEN-CHI Institute of Metal Research; Academia Sinica Smelting Works No. l; Ministry of Metal Industries |
|
Cite this article:
CHAO PEI-YING;LEE KENG-SHENG;FANG BING;TAN KWO YONG;WANG CHUEN-CHI Institute of Metal Research; Academia Sinica Smelting Works No. l; Ministry of Metal Industries. ON THE CONCENTRATION OF CADMIUM AND RECOVERY OF LEAD FROM THE LEAD BLAST FURNACE DUST. Acta Metall Sin, 1957, 2(1): 31-40.
|
|
|
Abstract On the basis of the distribution of lead, cadmium, arsenic and zinc amongthe various phases during the smelting process, the disadvantages of the currentlyadopted method using silica as slag-forming material for the treatment of leadblast furnace dust have been discussed. Experiments have been carried out in treating the dust with a new method,which is based upon the iron precipitation reaction with Na_2CO_3 as flux. Resultsobtained show: 1) 99.55% cadmium of the original dust may be concentrated intothe secondary dust; 2) 95.6% of lead may be recovered simultaneously, its purityis about 97%; 3) as cadmium in the secondary dust is easily leachable, a rate ofrecovery of cadmium as high as 98.5% could be obtained. It is suggested that,the present method, in view of its high recovery of valuable metals and its com-paratively simple operating procedure, is well suitable for the dust treatment inthe lead smelting industries.
|
|
Received: 18 January 1957
|
[1] 1949. 584. [2] OEEC Technical Assistance Mission, Zinc and Lead Smelting and Refining in U. S. A., 1955, Report No. 85, Vol. 2, 70--74. [3] Budgen, N. F., "Cadmium, Its Metallurgy, Ptoperties and Uses", 1924, 63. [4] 安斯林原著,沈曙东译,湿法回收烟尘中的铊与镉,有色金属,1955,6(总14期),17. [5] 李庚生、赵培英、方柄、谈国用等,湿法回收铅鼓风炉烟尘中的镉的研究,金属研究所研究报告,1955. [6] Smitheills, C. J., Metals Reference Book 1949, 418--455. [7] Kubaschewski, O. and Evans, E. Ll., Metallurgical Thermochemistry, 1951, 297、 305. [8] Gross, P. and Warrington, M., The Reduction of Zinc Sulphide by Iron under Reduced Pressure, Discussions of Faraday Society, No. 4 (1948) , 215. [9] Ono, K., Some Studies on the Smelting of Copper and Lead, The Science Reports of the Research Institutes, Tohoku University (Japan), Series A, 4 (1952) , 4, 416. [10] 契日科夫原著,傅崇说译,炼铅学,上册,1954,87、 88、 5. [11] 方柄、李庚生、赵培英、王文绍,从硫酸铅回收铅的研究,有色金属,1956,4(总24期),12. [12] 张开翥、王文绍,使用碳酸钠-铁屑法处理铅浮渣的试验初步总结,有色金属,1956,4(总24期),5. |