ON THE CONCENTRATION OF CADMIUM AND RECOVERY OF LEAD FROM THE LEAD BLAST FURNACE DUST
CHAO PEI-YING;LEE KENG-SHENG;FANG BING;TAN KWO YONG;WANG CHUEN-CHI Institute of Metal Research; Academia Sinica Smelting Works No. l; Ministry of Metal Industries
Cite this article: 

CHAO PEI-YING;LEE KENG-SHENG;FANG BING;TAN KWO YONG;WANG CHUEN-CHI Institute of Metal Research; Academia Sinica Smelting Works No. l; Ministry of Metal Industries. ON THE CONCENTRATION OF CADMIUM AND RECOVERY OF LEAD FROM THE LEAD BLAST FURNACE DUST. Acta Metall Sin, 1957, 2(1): 31-40.

Download:  PDF(870KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the basis of the distribution of lead, cadmium, arsenic and zinc amongthe various phases during the smelting process, the disadvantages of the currentlyadopted method using silica as slag-forming material for the treatment of leadblast furnace dust have been discussed. Experiments have been carried out in treating the dust with a new method,which is based upon the iron precipitation reaction with Na_2CO_3 as flux. Resultsobtained show: 1) 99.55% cadmium of the original dust may be concentrated intothe secondary dust; 2) 95.6% of lead may be recovered simultaneously, its purityis about 97%; 3) as cadmium in the secondary dust is easily leachable, a rate ofrecovery of cadmium as high as 98.5% could be obtained. It is suggested that,the present method, in view of its high recovery of valuable metals and its com-paratively simple operating procedure, is well suitable for the dust treatment inthe lead smelting industries.
Received:  18 January 1957     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1957/V2/I1/31

[1] 1949. 584.
[2] OEEC Technical Assistance Mission, Zinc and Lead Smelting and Refining in U. S. A., 1955, Report No. 85, Vol. 2, 70--74.
[3] Budgen, N. F., "Cadmium, Its Metallurgy, Ptoperties and Uses", 1924, 63.
[4] 安斯林原著,沈曙东译,湿法回收烟尘中的铊与镉,有色金属,1955,6(总14期),17.
[5] 李庚生、赵培英、方柄、谈国用等,湿法回收铅鼓风炉烟尘中的镉的研究,金属研究所研究报告,1955.
[6] Smitheills, C. J., Metals Reference Book 1949, 418--455.
[7] Kubaschewski, O. and Evans, E. Ll., Metallurgical Thermochemistry, 1951, 297、 305.
[8] Gross, P. and Warrington, M., The Reduction of Zinc Sulphide by Iron under Reduced Pressure, Discussions of Faraday Society, No. 4 (1948) , 215.
[9] Ono, K., Some Studies on the Smelting of Copper and Lead, The Science Reports of the Research Institutes, Tohoku University (Japan), Series A, 4 (1952) , 4, 416.
[10] 契日科夫原著,傅崇说译,炼铅学,上册,1954,87、 88、 5.
[11] 方柄、李庚生、赵培英、王文绍,从硫酸铅回收铅的研究,有色金属,1956,4(总24期),12.
[12] 张开翥、王文绍,使用碳酸钠-铁屑法处理铅浮渣的试验初步总结,有色金属,1956,4(总24期),5.
No related articles found!
No Suggested Reading articles found!