| AN INVESTIGATION OF CHEMICAL EQUILIBRIA IN THE BLAST-FURNACE HEARTH Ⅱ. THE SILICON-SULFUR, SILICON-CARBON AND SILICONMANGANESE EQUILIBRIA |
| CHOU YUAN-HSI Institute of Metallurgy and Ceramics; Academia Sinica |
|
Cite this article:
CHOU YUAN-HSI Institute of Metallurgy and Ceramics; Academia Sinica. AN INVESTIGATION OF CHEMICAL EQUILIBRIA IN THE BLAST-FURNACE HEARTH Ⅱ. THE SILICON-SULFUR, SILICON-CARBON AND SILICONMANGANESE EQUILIBRIA. Acta Metall Sin, 1957, 2(1): 19-30.
|
|
|
Abstract In a previous paper, it has been found that the manganese-sulfur equilibriumis approached in the blast-furnace hearth in agreement with the conelusions of somerecent publications. This paper presents an analysis of the same data used in theprevious paper with a view to investigating the equilibria batween silicon and theother components dissolved in liquid iron sach as salfur, carbon and manganese. It is shown that neither the silicon-sulfur nor the silicon-manganese equilibriumis approached in the blast-furnace hearth, although a parellel relationship existsbetween [%S]~(1/2)/(α_(SiO_2))~(1/2) and (%S)/[%S] and also between [%Si]~(1/2)/(α_(SiO_2))~(1/2)and [%Mn]/(%MnO). By using [%Si]~(1/2)/(α_(SiO_2))~(1/2) as an index ot the degree of silicon reduction,it has been found that an increase in slag basicity promotes silicon reduction in theblast-furnace hearth. Consequently, it is possible for the silicon-carbon reaction toapproach equilibrium in the blast-furnace hearth provided that basicity is highenough. The favorable effect of increasing basicity on the degree of silicon reduc-tion is briefly discussed from the view point of the mechanism of reduction.
|
|
Received: 18 January 1957
|
[1] 鄒元爔,金属学报,1(4) ,(1956) . [2] Joseph, T. L., Trans. Am. Min. Met. Engrs., 125, 204 (1937) . [3] Oelsen, W. Und Maetz, H., Stahl und Eisen, 69, 147 (1949) . [4] Chipman, J., Metal Progress, 62 (12) , 97 (1952) . [5] 鄒元爔,金属学报,1(2) ,127(1956) . [6] 鄒元爔,金属学报,1(2) ,143(1956) . [7] Fulton, J. C. and Chipman, J., J. Metals, 6 (10) , 1136 (1954) . [8] Filer, E. W. and Darken, L. S., Trans. Am. Min. Met. Engrs., 194, 253 (1952) . |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|