Please wait a minute...
Acta Metall Sin  1958, Vol. 3 Issue (2): 138-180    DOI:
Current Issue | Archive | Adv Search |
RESEARCH ON AUSTENITIC Cr-Mn-C-N STAINLESS STEELS
Hsiao Chi-mei Peking Institute of Ferrous Metallurgy
Cite this article: 

Hsiao Chi-mei Peking Institute of Ferrous Metallurgy. RESEARCH ON AUSTENITIC Cr-Mn-C-N STAINLESS STEELS. Acta Metall Sin, 1958, 3(2): 138-180.

Download:  PDF(10921KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Over 200 Cr-Mn-C-N experimental steels have been systematically studied bya combination of microscopic examination,X-ray diffraction,electrolytic extraction,chemical analysis,hardness and magnetic measurements,density and dilatometricmethods,oxidation test,tensile tests at both room-and elevated-temperatures,creep-rupture test,etc.,and the main findings are presented as follow:(1)Stable austenitic region.(2)Solid state reactions:martensitic transformation,precipitation reactions,and formation of sigma phase.(3)Room-and elevated-temperatures properties,and their relation to the che-mical composition of the steels.(4)Strengthening effect of interstitial solid solution.(5)Effect of precipitation reaction on elevated-temperature strength.(6)Effect of V,W,Mo,Nb,B and Si.(7)Tentative recommendation for indus rial applications.
Received:  18 February 1958     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1958/V3/I2/138

[1] C.M.Hsiao(萧纪美)and E.J.Dulis,Trans.ASM,49(1957) ,Preprint № 26(1956) .
[2] C.M.Hsiao(萧纪美)and E.J.Dulis,Trans.ASM,50(1958) ,Preprint № 29(1957) .
[3] C.M.Hsiao(萧纪美)and E.J.Dulis,Sym.“Relation of structure and High Temperature,Properties”,AIME(1957) .
[4] C.M.Hsiao(萧纪美)and E.J.Dulis,WADC Report,AF33(616) -3318,(Feb.1957) .
[5] C.M.Hsiao(萧纪美)and E.J.Dulis,Rep.Crucible Steel CO.of Am.,Proj.148,153(June,1957) .
[6] F.M.Becket,Yearbook,Am.Iron Steel Inst.(1930) ,173.
[7] W.K(o|¨)ster,Archiv Eisenhüttenwesen,7(1933-4) ,687-8.
[8] S.Gunzberg,N.A.Aleksandrova,and E.Geldermann,Archiv.Eisenhüttenweson,8(1933-4) ,121-3.
[9] M.Schmidt and H.Legat,Archiv.Eisenhüttenwesen,10(1936-7) ,297-303.
[10] H.Legat,Archiv Eisenhüttenweson,11(1937-8) ,337-41.
[11] C.O.Burgess and W.D.Forgeng,Trans.AIME,131(1938) ,277-98.
[12] F.Bruhl,Archiv.Eisenhüttenwesen,10(1936-7) ,243-55.
[13] #12
[14] #12
[15] V.N.Krivobok,Trans.ASM,23(1935) ,1.
[16] R.Franks,Trans.ASM,23(1935) ,968.
[17] E.W.Colbeck and R.P.Garner,J.Iron Steel Inst.,193,99.
[18] H.Krainer and O.Mirt,Archiv.Eisenhüttenwesen,15(1941-4) ,467-72.
[19] F.Rapatz,Stahl u Eisen,61(1941) ,1071-8.
[20] L.Schaeben,Korrosion u Metallschutz,19(1943) ,44-6.
[21] R.Franks,W.O.Binder,and J.Thompson,Trans.ASM,47(1955) ,231-66.
[22] E.J.Whittenberg,E.R.Rosenow,and D.J.Carney,Trans.AIME(1957) .
[23] V.F.Zackay,J.F.Carlson,and P.L.Jackson,Trans.ASM,48(1956) ,509-25.
[24] J.F.Carlson and V.F.Zackay,Trans.AIME,203(1955) ,112-3.
[25] U.S.Steel Co.,Materials and Method,45(1957,① ),104-5.
[26] G.F.Tisinai,J.K.Stanley,and C.H.Samans,Trans.ASM,48(1956) ,356-67.
[27] G.F.Tisinai and C.H.Samans,Trans.ASM,49(1957) ,preprint № 30(1956) .
[28] R.T.Howard and M.Cohen,Trans.AIME,172(1947) ,415-26.
[29] T.V.Simpkinson and M.J.Lavigue,Metal Progress(1949,② ),164-7.
[30] Bettelle Memorial Inst.,Rep.to Crucible St.Am.(1944) ,95.
[31] F.Larson and J.Miller,Trans.ASME,74(1952) ,756-61.
[32] W.T.DeLong,G.A.Ostrom,and E.R.Szumachowski,Welding Res.,21(1956,(11) ),521S-8S.
[33] R.H.Aborn and E.C.Bain,Trans.ASST,18(1930) ,837-73.
[34] G.H.Eichelman,Jr.and F.C.Hull,Trans.ASM,45(1953) ,77-104.
[35] F.C.Monkman,F.B.Cuff,Jr.and N.J.Grant,Metal Progress(1957,④ ),94-6.
[36] A.H.Geisler.Phase Transformation in Solids(1951) ,387-544.
[37] R.F.Mehl and C.S.Barrett,Trans.AIME,93(1931) ,78-110.
[38] H.J.Goldschmidt,J.Iron steel Inst.,160(1948) ,345-61.
[39] S.Erikssen,Jerh.Ann.(1934) ,503-43.
[40] A.Lockington and R.L.Samuel,Metal Treat.Drop Forging(1951 ⑨ ),407-15.
[41] L.K.Jetter and R.F.Mehl,Trans.AIME,152(1943) ,166-8.
[42] F.K.Bloom,G.N.Goller and P.G.Mabus,Trans.ASM,39(1947) ,843-67.
[43] A.R.Troiano and F.T.McGuire,Trans.ASM,31(1943) ,340-64.
[44] B.Cina,J.Iron Steel Inst.,177(1954) ,406-22.
[45] E.R.Parker and T.H.Hazlett,Relation of Properties to Microstructure,ASM(1954) ,30-70.
[46] H.Krainer,Archiv.Eisenh(a|¨)ttenwesen,22(1951) ,53-62.
[47] F.Wever and P.Rutten,Mitteilungen Kaiser-Wilhelm-Inst.Eisenforseh,6(1924-5) ,1-6.
[48] A.Westgren and G.Phragmén,J.Iron Steel Inst.,109(1924) ,159-74.
[49] O.Eisenhut and E.Kaupp,Z.Elektrochem.,36(1920) ,392-404.
[50] E (O|¨)hman,Z.Phys.Chem.,8(1930) ,81-110.
[51] N.P.Allen,T.H.Schofield and A.E.L.Tate,Nature,168(1951) ,378-9.
[52] J E.Dorn,P.Pietrokowsky and T.E.Tietz,J.Metals,188(1950) ,933-43.
[53] L Pauling,The Nature of the Chemical Bond(1940) ,58-65.
[54] Gordy,Phys.Rev.,69(1946) ,604-7.
[55] F Laves,Theory of Alloy Phases,ASM(1956) ,131.
[56] H.D.Newell and M.Fleischmann,U.S.Patent 2,118,683(1938) .
[57] A.L.Schaeffer,Welding J.,20(1947) ,601S-620S.
[58] R.H.Thielemann,Proc.ASTM,40(1940) ,788-804.
[59] C.B.Post and W.S.Eberly,Trans.ASM,39(1947) ,868-90.
[60] W.F.Simmons,V.N.Krivobok,N.L.Mochel,and R.Franks,ASTM,Sp.Pub.,№ 170(1957) .
No related articles found!
No Suggested Reading articles found!