| RESEARCH ON AUSTENITIC Cr-Mn-C-N STAINLESS STEELS |
| Hsiao Chi-mei Peking Institute of Ferrous Metallurgy |
|
Cite this article:
Hsiao Chi-mei Peking Institute of Ferrous Metallurgy. RESEARCH ON AUSTENITIC Cr-Mn-C-N STAINLESS STEELS. Acta Metall Sin, 1958, 3(2): 138-180.
|
|
|
Abstract Over 200 Cr-Mn-C-N experimental steels have been systematically studied bya combination of microscopic examination,X-ray diffraction,electrolytic extraction,chemical analysis,hardness and magnetic measurements,density and dilatometricmethods,oxidation test,tensile tests at both room-and elevated-temperatures,creep-rupture test,etc.,and the main findings are presented as follow:(1)Stable austenitic region.(2)Solid state reactions:martensitic transformation,precipitation reactions,and formation of sigma phase.(3)Room-and elevated-temperatures properties,and their relation to the che-mical composition of the steels.(4)Strengthening effect of interstitial solid solution.(5)Effect of precipitation reaction on elevated-temperature strength.(6)Effect of V,W,Mo,Nb,B and Si.(7)Tentative recommendation for indus rial applications.
|
|
Received: 18 February 1958
|
[1] C.M.Hsiao(萧纪美)and E.J.Dulis,Trans.ASM,49(1957) ,Preprint № 26(1956) . [2] C.M.Hsiao(萧纪美)and E.J.Dulis,Trans.ASM,50(1958) ,Preprint № 29(1957) . [3] C.M.Hsiao(萧纪美)and E.J.Dulis,Sym.“Relation of structure and High Temperature,Properties”,AIME(1957) . [4] C.M.Hsiao(萧纪美)and E.J.Dulis,WADC Report,AF33(616) -3318,(Feb.1957) . [5] C.M.Hsiao(萧纪美)and E.J.Dulis,Rep.Crucible Steel CO.of Am.,Proj.148,153(June,1957) . [6] F.M.Becket,Yearbook,Am.Iron Steel Inst.(1930) ,173. [7] W.K(o|¨)ster,Archiv Eisenhüttenwesen,7(1933-4) ,687-8. [8] S.Gunzberg,N.A.Aleksandrova,and E.Geldermann,Archiv.Eisenhüttenweson,8(1933-4) ,121-3. [9] M.Schmidt and H.Legat,Archiv.Eisenhüttenwesen,10(1936-7) ,297-303. [10] H.Legat,Archiv Eisenhüttenweson,11(1937-8) ,337-41. [11] C.O.Burgess and W.D.Forgeng,Trans.AIME,131(1938) ,277-98. [12] F.Bruhl,Archiv.Eisenhüttenwesen,10(1936-7) ,243-55. [13] #12 [14] #12 [15] V.N.Krivobok,Trans.ASM,23(1935) ,1. [16] R.Franks,Trans.ASM,23(1935) ,968. [17] E.W.Colbeck and R.P.Garner,J.Iron Steel Inst.,193,99. [18] H.Krainer and O.Mirt,Archiv.Eisenhüttenwesen,15(1941-4) ,467-72. [19] F.Rapatz,Stahl u Eisen,61(1941) ,1071-8. [20] L.Schaeben,Korrosion u Metallschutz,19(1943) ,44-6. [21] R.Franks,W.O.Binder,and J.Thompson,Trans.ASM,47(1955) ,231-66. [22] E.J.Whittenberg,E.R.Rosenow,and D.J.Carney,Trans.AIME(1957) . [23] V.F.Zackay,J.F.Carlson,and P.L.Jackson,Trans.ASM,48(1956) ,509-25. [24] J.F.Carlson and V.F.Zackay,Trans.AIME,203(1955) ,112-3. [25] U.S.Steel Co.,Materials and Method,45(1957,① ),104-5. [26] G.F.Tisinai,J.K.Stanley,and C.H.Samans,Trans.ASM,48(1956) ,356-67. [27] G.F.Tisinai and C.H.Samans,Trans.ASM,49(1957) ,preprint № 30(1956) . [28] R.T.Howard and M.Cohen,Trans.AIME,172(1947) ,415-26. [29] T.V.Simpkinson and M.J.Lavigue,Metal Progress(1949,② ),164-7. [30] Bettelle Memorial Inst.,Rep.to Crucible St.Am.(1944) ,95. [31] F.Larson and J.Miller,Trans.ASME,74(1952) ,756-61. [32] W.T.DeLong,G.A.Ostrom,and E.R.Szumachowski,Welding Res.,21(1956,(11) ),521S-8S. [33] R.H.Aborn and E.C.Bain,Trans.ASST,18(1930) ,837-73. [34] G.H.Eichelman,Jr.and F.C.Hull,Trans.ASM,45(1953) ,77-104. [35] F.C.Monkman,F.B.Cuff,Jr.and N.J.Grant,Metal Progress(1957,④ ),94-6. [36] A.H.Geisler.Phase Transformation in Solids(1951) ,387-544. [37] R.F.Mehl and C.S.Barrett,Trans.AIME,93(1931) ,78-110. [38] H.J.Goldschmidt,J.Iron steel Inst.,160(1948) ,345-61. [39] S.Erikssen,Jerh.Ann.(1934) ,503-43. [40] A.Lockington and R.L.Samuel,Metal Treat.Drop Forging(1951 ⑨ ),407-15. [41] L.K.Jetter and R.F.Mehl,Trans.AIME,152(1943) ,166-8. [42] F.K.Bloom,G.N.Goller and P.G.Mabus,Trans.ASM,39(1947) ,843-67. [43] A.R.Troiano and F.T.McGuire,Trans.ASM,31(1943) ,340-64. [44] B.Cina,J.Iron Steel Inst.,177(1954) ,406-22. [45] E.R.Parker and T.H.Hazlett,Relation of Properties to Microstructure,ASM(1954) ,30-70. [46] H.Krainer,Archiv.Eisenh(a|¨)ttenwesen,22(1951) ,53-62. [47] F.Wever and P.Rutten,Mitteilungen Kaiser-Wilhelm-Inst.Eisenforseh,6(1924-5) ,1-6. [48] A.Westgren and G.Phragmén,J.Iron Steel Inst.,109(1924) ,159-74. [49] O.Eisenhut and E.Kaupp,Z.Elektrochem.,36(1920) ,392-404. [50] E (O|¨)hman,Z.Phys.Chem.,8(1930) ,81-110. [51] N.P.Allen,T.H.Schofield and A.E.L.Tate,Nature,168(1951) ,378-9. [52] J E.Dorn,P.Pietrokowsky and T.E.Tietz,J.Metals,188(1950) ,933-43. [53] L Pauling,The Nature of the Chemical Bond(1940) ,58-65. [54] Gordy,Phys.Rev.,69(1946) ,604-7. [55] F Laves,Theory of Alloy Phases,ASM(1956) ,131. [56] H.D.Newell and M.Fleischmann,U.S.Patent 2,118,683(1938) . [57] A.L.Schaeffer,Welding J.,20(1947) ,601S-620S. [58] R.H.Thielemann,Proc.ASTM,40(1940) ,788-804. [59] C.B.Post and W.S.Eberly,Trans.ASM,39(1947) ,868-90. [60] W.F.Simmons,V.N.Krivobok,N.L.Mochel,and R.Franks,ASTM,Sp.Pub.,№ 170(1957) . |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|