THE FREE ENERGIES OF FORMATION OF Mg_3Bi_2, Ca_3Bi_2, CaMg_2Bi_2 AND K_9Mg_6Bi_7
CHOU YUAN-HSI (Institute of Metallurgy; Academic Sinica)
Cite this article: 

CHOU YUAN-HSI (Institute of Metallurgy; Academic Sinica). THE FREE ENERGIES OF FORMATION OF Mg_3Bi_2, Ca_3Bi_2, CaMg_2Bi_2 AND K_9Mg_6Bi_7. Acta Metall Sin, 1964, 7(2): 217-219.

Download:  PDF(212KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 February 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I2/217

[1] 邹元爔:待发表.
[2] Egan, J. J.: Acta Met., 1959, 7, 8, 560.
[3] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) , p. 859.
[4] Kubaschewski, O., Walter, A.: Z. Elektrochem., 1939, 45, 630, 732.
[5] Davey, T. R. A.: Trans AIME, 1956, 206, 341.
[6] Strickler, H. S., Seltz, H.: J. Am. Chem. Soc., 1936, 58, 2084.
[7] Kubaschewski, O., Evans, E. L.: Metallurgical Thermochemistry, 2nd ed., (Pergamon, 1955) , p. 33.
[8] 郑文陞、邹元爔:金属学报,1964,7,130.
[9]#12
No related articles found!
No Suggested Reading articles found!