THE FREE ENERGIES OF FORMATION OF Mg_3Bi_2, Ca_3Bi_2, CaMg_2Bi_2 AND K_9Mg_6Bi_7 |
CHOU YUAN-HSI (Institute of Metallurgy; Academic Sinica) |
|
Cite this article:
CHOU YUAN-HSI (Institute of Metallurgy; Academic Sinica). THE FREE ENERGIES OF FORMATION OF Mg_3Bi_2, Ca_3Bi_2, CaMg_2Bi_2 AND K_9Mg_6Bi_7. Acta Metall Sin, 1964, 7(2): 217-219.
|
|
Received: 18 February 1964
|
[1] 邹元爔:待发表. [2] Egan, J. J.: Acta Met., 1959, 7, 8, 560. [3] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) , p. 859. [4] Kubaschewski, O., Walter, A.: Z. Elektrochem., 1939, 45, 630, 732. [5] Davey, T. R. A.: Trans AIME, 1956, 206, 341. [6] Strickler, H. S., Seltz, H.: J. Am. Chem. Soc., 1936, 58, 2084. [7] Kubaschewski, O., Evans, E. L.: Metallurgical Thermochemistry, 2nd ed., (Pergamon, 1955) , p. 33. [8] 郑文陞、邹元爔:金属学报,1964,7,130. [9]#12 |