Acta Metall Sin  1964, Vol. 7 Issue (2): 189-216    DOI:
Current Issue | Archive | Adv Search |
TRANSMISSION ELECTRON MICROSCOPY OF PHASE TRANSFORMATION IN METALS AND ALLOYS
KUO KE-HSIN(Institute of Metal Research; Academia Sinica)
Cite this article: 

KUO KE-HSIN(Institute of Metal Research; Academia Sinica). TRANSMISSION ELECTRON MICROSCOPY OF PHASE TRANSFORMATION IN METALS AND ALLOYS. Acta Metall Sin, 1964, 7(2): 189-216.

Download:  PDF(14887KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 February 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I2/189

[1] Thomas, G.: Transmission Electron Microscopy of Metals, (Wiley, 1962) .
[2] Journal of the Institute of Metals: Symposium on "The Application of Thin-Film Techniques to the Electron-Microscopic Examination of Metals" 1958-59, 87, 385-458.
[3] Houwink, A. L., Spit, B. J.: The Proccedings of the European Regional Conference on Electron Microscopy, Delft, 1960, (De Nederlandse Vereniging voor Electronenmicrosc0pie, 1961) , vol. 1.
[4] Breese, S. S. Jr.: Fifth International Congress for Electron Microscopy, (Academic, 1962) , vol. 1.
[5] Thomas, G., Washburn, J.: Electron Microscopy and Strength of Crystals, (Interscience, 1963) .
[6] 电子显微鏡(直接观察)特集号:日本金属学会会报,1963,2,119.
[7] Nicholson, R. B., Thomas, G., Nutting, J.: J. Inst. Metals, 1958-59, 87, 429.
[8] Polmear, I. J.: J. Australian Inst. Metals, 1962, 7, 50.
[9] Thomas, G.: Electron Microscopy and Strength of Crystals, ed. G. Thomas, J. Washburn, (Interscience, 1963) , p. 793.
[10] Nicholson, R. B.: Electron Microscopy and Strength of Crystals, ed. G. Thomas, J. Washburn, (Interscience, 1963) , p. 861.
[11] 幸田成康:电子显微鏡(直接观察)特集号:日本金属学会会报,1963,2,139.
[12] Kelly, A., Nicholson, R. B.: Progress in Metal Physics, (Pergamon, 1963) , vol. 10, No. 3.
[13] Nicholson, R. B., Nutting, J.: Phil. Mag., 1958, 3, 531. (Al-Cu).
[14] Thomas, G., Nutting, J.: Acta Met., 1959, 7, 515. (Al-Cu).
[15] Thomas, G., Whelan, M. J.: Phil. Mag., 1961, 6, 1103. (Al-Cu).
[16] Deschamps, P.: J. Phys. Radium, 1962, 23, 807. (Al-Cu).
[17] Heimendahl, M., Wassermann, G.: Z. Metallk., 1962, 58, 275. (Al-Cu). Heimendahl, M., Wassermann, G.: Z. Metallk., 1963, 54, 385. (Al-Cu).
[18] Nicholson, R. B.: The Proccedings of the European Regional Conference on Electron Microscopy, Delft, 1960, ed. A. L. Houwink, B. J. Spit, (De Nederlandse Vereniging voor Electronenmicroscopie, 1961) , vol. 1, p. 375. (Al-Cu, Al-Ag).
[19] Bonar, L. G., Kelly, A.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-11. (Al-Cu).
[20] Takahashi, N.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, HH-1. (Al-Cu, Al-Ag).
[21] Koda, S., Matsuura, K., Takahashi, S.: J. Inst. Metals, 1962--63, 91, 229. (Al-Cu).
[22] Koda, S., Matsuura, K., Nemoto, M.: J. Australian Inst. Metals, 1963, 8, 197. (Al-Cu).
[23] Reimer, L.: Z. Metallk., 1959, 50, 606. (Al-Ag).
[24] Freise, E. J., Kelly, A., Nicholson, R. B.: Acta Met., 1961, 9, 250. (Al-Ag).
[25] Nicholson, R. B., Nutting, J.: Acta Met., 1961, 9, 332. (Al-Ag).
[26] Frank, G. R. Jr., Robinson, D. L., Thomas, G.: J. Appl. Phys., 1961, 32, 1763. (Al-Ag)..
[27] Takahashi,N.,高桥 昇:电子显微鏡,1959,8,1. (Al-Ag,Al-Cu.Sn-Sb).
[28] Takahashi, N.: Compt. Rend., 1962, 255, 2391. (Al-Ag).
[29] Hren, J. A., Thomas, G.: Trans. AIME, 1963, 227, 308. (Al-Ag). Hren, J. A., Thomas, G.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-1. (Al-Ag).
[30] Nicholson, R. B.: J. Phys. Radium, 1962, 23, 824. (Al-Ag, Al-Mg).
[31] Dupouy, G., Perrier, F., Takahashi, N.: Compt. Rend., 1963, 256, 545. (Al-Ag).
[32] Embury, J. D., Nicholson, R. B.: Acta Met., 1963, 11, 347. (Al-Mg).
[32a] McEvily, A. J., Snyder, R. L., Clark, J. B.: Trans. AIME, 1963, 227, 452. (Al-Mg).
[33] Saulnier, A.: Mem. Sci. Rev. Met., 1961, 58, 615. (Al-Si).
[34] Genty, B., Graf, R., Lenoir, G.: Compt. Rend., 1958, 247, 1731. (Al-Zn-Mg).
[35] Thomas, G.: Phil. Mag., 1959, 4, 606. (Al-Zn-Mg).
[36] Thomas, G., Nutting, J.: J. Inst. Metals, 1959--60, 88, 81. (Al-Zn-Mg).
[37] Nicholson, R. B., Thomas, G., Nutting, J.: Acta Met., 1960, 8, 172. (Al-Zn-Mg, Al-Cu).
[38] Thomas, G.: J. Inst. Metals, 1961-62, 90, 57. (Al-Mg-Si).
[39] Murakami, Y., Kawano, O.: Trans. Japan Inst. Metals, 1960, 1, 27, (Al-Mg-Si, Al-Cu-Mg, Al-Zn-Mg).
[39a] 太田陆奥雄:日本金属学会志,1963,27,197. (Al-Cu-Mn)。
[40] Leslie, W. C.: Acta Met., 1961, 9, 1004. (Fe-C, Fe-Mn-C).
[41] Smith, E., Direct Observation of Imperfections in Crystals, ed. J. B. Newkirk, J. H. Wernick. (Interscience, 1962) , p. 203. (Fe-C).
[42] Pitsch, W.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, HH-2. (Fe-Mn-C). Pitsch, W.: Arch. Eisenhuttenw., 1963, 381. (Fe-Mn-C).
[43] McLean, D.: The Proccedings of the European Regional Conference on Electron Microscopy, Delft, 1960, ed. A. L. Houwink, B. J. Spit, (De Nederlandse Vereniging voor Electronenmicroscopie, 1961) , vol. 1, p. 425. (Fe-C).
[44] Gielen, P., Greday, T.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, CC-5. (Fe-Nb-C).
[44a] Morrison, W. B.: J. Iron Steel Inst. (London), 1963, 201, 317. (Fe-Mn-Nb-C).
[45] Phillips, V. A.: Acta Met., 1963, 11, 1139. (Fe-C-N).
[46] Pitsch, W.: The Proccedings of the European Regional Conference on Electron Microscopy, Delft, 1960, ed. A. L. Houwink, B. J. Spit, (De Nederlandse Vereniging voor Electronenmicroscopie, 1961) , vol. 1, p. 498. (Fe-N).
[47] Booker, G. R.: Acta Met., 1961, 9, 590. (Fe-N).
[48] Keh, A. S., Wriedt, H. A.: Trans. AIME, 1962, 224, 560. (Fe-N).
[49] Hale, K. F., McLean, D.: J. Iron Steel Inst. (London), 1963, 201, 337. (Fe-C, Fe-N).
[50] Hatwell, H., Votava, E.: Acta Met., 1961, 9, 945. (不锈鋼).
[51] Haddrill, D. M., Younger, R. N., Baker, R. G.: Acta Met., 1961, 9, 982. (不銹鋼).
[52] Garofalo, F., Gemmingen, F., Domis, W. F.: Trans. Am. Soc. Metals, 1961, 54, 430. (不銹鋼).
[53] 成田貴一、高桥荣冶:日本金属学会志,1962,26,639. (不銹鋼)。
[54] Aswegen, J. S. T., Honeycombe, R. W. K.: Acta Met., 1962, 10, 262. (不銹鋼). Aswegen, J. S. T., Honeycombe, R. W. K.: Fifth International Congress for Electron Micrnscopy, ed. S.S. Jr. Breese, (Academic, 1962) , vol. 1, CC-2. (不銹鋼).
[55] Younger, R. N., Haddrill, D. M., Baker, R. G.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, CC-3. (不銹鋼).
[56] Picketing, F. B., Burns, K. W., Keown, S. R.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, CC-4. (不銹鋼).
[57] Silcock, J. M.: J. Iron Steel Inst., 1963, 201, 409. (不銹鋼).
[58] Hornbogen, E.: Z. Metallk., 1961, 52, 47. (Fe-Mo, Fe-W).
[59] Hornbogen, E.: Acta Met., 1962, 10, 525. (Fe-Cu, Fe-Au). Hornbogen, E.: Acta Met., 1962, 10, 1187. (Fe-Cu, Fe-Au).
[60] Hornbogen, E.: Trans. Am. Soc. Metals, 1962, 55, 719. (Fe-P).
[61] Speich, G. R.: Trans. AIME, 1962, 224, 850. (Fe-Nb, Fe-Ti).
[61a] Speich, G. R.: Trans. AIME, 1963, 227, 754. (Fe-Ni-Ti).
[62] Saulnier, A., Mirand, P.: Mem. Sci. Rev. Met., 1960, 57, 91. (Cu-Be, Al-Mg).
[63] Armitage, W. K., Kelly, P. M., Nutting, J.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-4. (Cu-Be).
[64] Tanaka, K., Mannami, M., Izumi, K., Marukawa, K.: Acta Met., 1963, 11, 79. (Cu-Be).
[65] Price, R. J., Kelly, A.: Acta Met., 1963, 11, 915. (Cu-Be).
[66] Phillips, V. A., Livingston, J. D.: Phil. Mag., 1962, 7, 969. (Cu-Co).
[67] Ashby, M. F., Brown, L. M.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-5. (Cu-Co).
[68] Phillips, V. A.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-10. (Cu-Co).
[69] Buckle, M. C., Manenc, J.: Mem. Sci. Rev. Met., 1960, 57, 435. (Cu-Ti).
[70] Ashby, M. F.: Fifth International Congress for Electron Microscopy, ed. S. S. Jr. Breese, (Academic, 1962) , vol. 1, K-6. (Cu-氧化物). Ashby, M. F.: Electron Microscopy and Strength of Crystals, ed. G. Thomas, J. Washburn, (Interscience,
No related articles found!
No Suggested Reading articles found!