KINETICS OF THE REACTIONS BETWEEN LIQUID SLAGS AND CARBON-SATURATED IRON
WANG WEI-YUAN(Institute of Metallurgy; Academia Sinica)
Cite this article: 

WANG WEI-YUAN(Institute of Metallurgy; Academia Sinica). KINETICS OF THE REACTIONS BETWEEN LIQUID SLAGS AND CARBON-SATURATED IRON. Acta Metall Sin, 1964, 7(4): 376-382.

Download:  PDF(550KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation of the kinetics of the reactions between liquid slags and carbonsaturated iron including the reduction of FeO, MnO, CrO and V_2O_3 by carbon and the desulphurization of iron leads to the conclusion that the chemical reactions come to equilibrium rapidly at the slag-metal interface, while the controlling step is convective diffusion. It has been found that the reactions are of the first order when the melt is kept in a rotational motion, caused by the use of a rotating crucible or stirrer, and are of second order when the melt is kept in a stationary crucible and stirred by CO gas bubbles only. The thickness of the diffusion boundary layer δ, obtained from a treatment of Chipman's desulphurization data and Philbrook's data on the reduction of FeO, which correspond to the two fore-mentioned cases respectively, has been found to be inversely propertional to ω~(1/2), the square root of the angular velocity, and C_(FeO), the concentration of FeO in the slag phase.The present problem has been treated on the basis of the principle of convective diffusion across a solid-liquid interface according to Levich. It has been found that our findings can be satisfactorily explained by an application of this principle. An exceptional case is the reduction of SiO_2 from slags, which is probably controlled by interfacial chemical reaction.
Received:  18 April 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I4/376

[1] Dancy, T. E.: J. Iron Steel Inst. (London), 1951, 169, 17.
[2] Philbrook, W. O., Kirkbride, L. D.: Trans. AIME, 1956, 206, 351.
[3] Goldman, K. M., Chang Lo-ching (张祿经): Trans. AIME, 1948, 176, 309.
[4] Ramachandran, S., King, T. B., Grant, N. J.: Trans. AIME, 1956, 206. 1549.
[5] Fulton, J. C., Chipman, J.: The Physical Chemistry of Steelmaking, ed. J. F. Elliott, (Wiley, 1958) , p. 113.
[6] 沢村企好:铁钢,1958,44,215.
[7] #12
[8] McCoy, C. W., Philbrook, W. O.: Trans. AIME, 1958, 212, 226.
[9] 王渭源、邹元爔:科学通报,1962,(1) ,28.
[10] 赵彭年、邹元爔:金属学报,1963,6,29.
[11] Tarby, S. K., Philbrook, W. O.: J. Metals, 1961, 13, 442.
[12] #12
[13] Wagner, C.: The Physical Chemistry of Steelmaking, ed. J. F. Elliott, (Wiley, 1958) , p. 237.
[14] #12
[15] Fulton, J. C., Chipman, J.: Trans. AIME,, 1959, 215, 888.G
No related articles found!
No Suggested Reading articles found!