STUDIES ON THE VOLATILITY OF SnO IN THE SnO-SiO_2 SYSTEM
LI CHEN-CHIA(Kunming Institute of Technology) LU AI-CHUN; SUN NGO-TING(Institute of Precious Metals; Academia Sinica)
Cite this article: 

LI CHEN-CHIA(Kunming Institute of Technology) LU AI-CHUN; SUN NGO-TING(Institute of Precious Metals; Academia Sinica). STUDIES ON THE VOLATILITY OF SnO IN THE SnO-SiO_2 SYSTEM. Acta Metall Sin, 1964, 7(4): 383-390.

Download:  PDF(715KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Rates of volatilization of SnO from the binary silicate melts containing 60.60 to 91.00 wt.-% SnO were measured by the "Loss Weight" method. It was found that the logarithm of volatilization rate or vapour pressure of SnO is proportional to the composition of the melt. From these experimental results the activities of SnO and SiO_2 were calculated, and it occurred that they exhibit considerable negative deviation from Raoult's Law. Since the rate of volatilization varies exponentially with the SnO content in the binary melt, it is unlikely that this deviation is associated with the formation of compound between. SnO and SiO_2.
Received:  18 April 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I4/383

[1] Schuhmann, R., Ensio, P. J.: Trans. AIME, 1951, 191, 401.
[2] Richardson, F. D., Webb, L. E.: Trans. Inst. Mining Met., (London), 1955, 64, 529.
[3] Fulton, J. C., Chipman, J.: Trans. AIME, 1954, 200, 1136.
[4] 邹元爔:金属学报,1956,1,127.
[5] Chou Yuan-hsi(邹元爔), Chao Peng-nian (赵彭年): Sci. Sinica, 1962, 11, 1287.
[6] Keysselitz, B., Kohlmeyer, E. J.: Z. Erzbergbau Metallhuettenw., 1933, 30, 185.
[7] 冶金文摘,1962,(8) ,第四分册,14.
[8] #12
[9] Spandau, H., Kohlmeyer, E. J.: Z. Anorg. Chem., 1947, 254, 65.
[10] Callow, R. J.: Trans. Faraday Soc., 1950, 46, 663.
[11] Preston, E., Turner, W. E. S.: J. Soc. Glass Technol., 1932, 16, 331.
[12] Preston, E., Turner, W. E. S.: J. Soc. Glass Technol., 1933, 17, 122.
[13] Preston, E., Turner, W. E. S.: J. Soc. Glass Technol., 1934, 18, 143.
[14] Alcock, C. B., Hooper, G. W.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 1, p. 325.
[15] (1962) , 2.h
No related articles found!
No Suggested Reading articles found!