AN INVESTIGATION OF VISCOSITY, FUSIBILITY AND MINERAL CONSTITUTION OF BLAST-FURNACE TITANOSLAGS
MOK PUI-KUN; CHEN CHUNG-SHAN(Institute of Metallurgy; Academia Sinica)
Cite this article: 

MOK PUI-KUN; CHEN CHUNG-SHAN(Institute of Metallurgy; Academia Sinica). AN INVESTIGATION OF VISCOSITY, FUSIBILITY AND MINERAL CONSTITUTION OF BLAST-FURNACE TITANOSLAGS. Acta Metall Sin, 1964, 7(4): 363-375.

Download:  PDF(2575KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The viscosity of slags containing Al_2O_3 15%, MgO 10%, TiO_2 15—35% and with a CaO/SiO_2 ratio of 0.6—1.6 has been measured with an oscillating viscosimeter. Experimental results indicate that the viscosity of titanoslags is very low provided they are not previously subjected to a strong reducing action. The melting point of the slags depends on the CaO/SiO_2 ratio and TiO_2 content. Under a strong reducing condition, however, the TiO_2 can be reduced to lower oxides and even titanium carbide, and the slags become, quite viscous. An increase of temperature and decrease of CaO/SiO_2 ratio increase the rate of thickening. Experimental evidence verifies the presence of finelydispersed titanium carbide, which is the primary cause for thickening. The addition of an oxidizing agent or blowing of slightly oxidizing gases such as CO+CO_2 through the slag can prevent the latter from becoming viscous. These measures might prove helpful in blast-furnace smelting of titanium-containing iron ores.The main mineral constituents of the titanoslgs under investigation are perovskite, anosovite, baikovite and titaniferrous augite. Their relative amount depends upon the chemical composition of the slags and the degree of reduction.
Received:  18 April 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I4/363

[1] #12
[2] #12
[3] #12
[4] #12
[5] #12
[6] #12
[7] Towers, H., Kay, J.: Trans. Brit. Ceram. Soc., 1950, 49, 341.
[8] #12
[9] #12
[10] #12
[11] #12
[12] Turnbull, R. C., Lawrence, W. G.: J. Am. Ceram. Soc., 1952, 35, 48.
[13] Ross, H. U.: Blast Furnace, Coke Oven, Rew Mater. Comm. Proc., 1958, 17, 47.
No related articles found!
No Suggested Reading articles found!