THE TRANSFORMATION OF CYANIDED 18CrMnTi and 18CrMnMo STEELS |
LU KUANG-HSI Kirin Institute of Technology |
|
Cite this article:
LU KUANG-HSI Kirin Institute of Technology. THE TRANSFORMATION OF CYANIDED 18CrMnTi and 18CrMnMo STEELS. Acta Metall Sin, 1965, 8(1): 82-133.
|
Abstract The C-curves of the cyanided case of 18CrMnTi and 18CrMnMo steels austeni-tized at 860℃ were determined by metallographic methods. In order to investigate theinfluence of nitrogen on the transformation characteristics, carburized samples with prac-tically the same carbon content as the cyanided ones were also prepared and examined. The results show that the cyanided samples have lower A_1 temperatures, considerablyhigher M_s points and shorter incubation periods in both the pearlitic and bainitic regionsthan the carburized samples. It is found that before the pearlitic and upper-bainitic reactions, a pro-cutectoid orpro-bainitic phase is precipitated along the austenite grain boundaries in the cyanidedsamples; and it is thought that this is likely a nitrogen-bearing phase which provides thephase boundary effect for the nucleation of the reactions and impoverishes the parentaustenite in alloy content, thus accelerating the transformation of austenite.
|
Received: 18 January 1965
|
[1] Houdremont, E., 1960, 2, 1418--1419, 1443--1447. [2] Rapatz, F., Mirt, O.: Stahl Eisen 1954, 1195. [3] Digges, T. G., Reinhart, F. M.: Trans. Am. Soc. Metals, 1948, 40. 1124. [4] Greninger, A. B., Troiano, A. R.: Trans. Am. Soc. Metals 1940, 28, 537. [5] #12 [6] Bose, B. N., Hawkes, M. F.: Trans, AIME 1950, 188. 307. [7] Просвирин,В.И,Энтин,С.Д.著,何忠治、欧阳可强译:马氏体的等温形成,(冶金工业出版社,1957年),6页. [8] Jolivet, H.: J. Iron Steel Inst., (London), 1939, 140, 95. [9] Lyman, T., Troiano, A. R.: Trans. Am. Soc. Metals, 1946, 37, 402. [10] Wever, F., Koch, W.: Stahl Eisen, 1954, 989. [11] #12 [12] Kehl, G. L.: The Principles of Metallographic Laboratory Practice, 3rd ed., (McGraw-Hill, 1949) , p. 417. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|