Please wait a minute...
Acta Metall Sin  1979, Vol. 15 Issue (4): 506-591    DOI:
Current Issue | Archive | Adv Search |
THE DISSOLUTION AND PRECIPITATION OF BORON CONSTITUENT AND THEIR EFFECTS ON THE PROPERTIES OF 40MnB STEEL
Res. Gp. of Boron Steels; Beijing Steel Works and Central Iron and Steel Research Institute; Ministry of Metallurgical Industry
Cite this article: 

Res. Gp. of Boron Steels; Beijing Steel Works and Central Iron and Steel Research Institute; Ministry of Metallurgical Industry. THE DISSOLUTION AND PRECIPITATION OF BORON CONSTITUENT AND THEIR EFFECTS ON THE PROPERTIES OF 40MnB STEEL. Acta Metall Sin, 1979, 15(4): 506-591.

Download:  PDF(2610KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of dissolution and precipitation of M_(23)(C,B)_6 during heating athigh temperature and cooling subsequently upon the properties of medium carbonsteel 40MnB containing different amounts of boron have been investigated by meansof quantitative phase analysis and boron-autoradiography. The volume fraction andgrain size of M_(23)(C,B)_6 precipitate may be increased with the increase of boroncontent and with the decrease of cooling rate. Although the steels contained dif-ferent amounts of boron, a same critical cooling rate may be appeared at whichM_(23)(C,B)_6 precipitate reached to saturation. The dissolution and precipitation ofM_(23)(C,B)_6 are deeply affected the hardenability and toughness of the steels. Underthe same condition, M_(23)(C,B)_6 in steels containing less boron may be precipitatedout in smaller size and easily dissolved. Thus, they exhibited better combinedproperties and less sensitivity to the change of heat history. Suggestion on stabi-lizing the properties of the steels has been made.
Received:  18 April 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I4/506

No related articles found!
No Suggested Reading articles found!