| THE DISSOLUTION AND PRECIPITATION OF BORON CONSTITUENT AND THEIR EFFECTS ON THE PROPERTIES OF 40MnB STEEL |
| Res. Gp. of Boron Steels; Beijing Steel Works and Central Iron and Steel Research Institute; Ministry of Metallurgical Industry |
|
Cite this article:
Res. Gp. of Boron Steels; Beijing Steel Works and Central Iron and Steel Research Institute; Ministry of Metallurgical Industry. THE DISSOLUTION AND PRECIPITATION OF BORON CONSTITUENT AND THEIR EFFECTS ON THE PROPERTIES OF 40MnB STEEL. Acta Metall Sin, 1979, 15(4): 506-591.
|
|
|
Abstract The effects of dissolution and precipitation of M_(23)(C,B)_6 during heating athigh temperature and cooling subsequently upon the properties of medium carbonsteel 40MnB containing different amounts of boron have been investigated by meansof quantitative phase analysis and boron-autoradiography. The volume fraction andgrain size of M_(23)(C,B)_6 precipitate may be increased with the increase of boroncontent and with the decrease of cooling rate. Although the steels contained dif-ferent amounts of boron, a same critical cooling rate may be appeared at whichM_(23)(C,B)_6 precipitate reached to saturation. The dissolution and precipitation ofM_(23)(C,B)_6 are deeply affected the hardenability and toughness of the steels. Underthe same condition, M_(23)(C,B)_6 in steels containing less boron may be precipitatedout in smaller size and easily dissolved. Thus, they exhibited better combinedproperties and less sensitivity to the change of heat history. Suggestion on stabi-lizing the properties of the steels has been made.
|
|
Received: 18 April 1979
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|