INTERACTIONS BETWEEN CREEP AND LOW CYCLE FATIOUE IN A NICKEL BASE SUPERALLOY
Zhang Anqing;Kong Qingping;Shi Changxu(Shih Chang-hsu) Institute of Metal Research; Academia Sinica
Cite this article: 

Zhang Anqing;Kong Qingping;Shi Changxu(Shih Chang-hsu) Institute of Metal Research; Academia Sinica. INTERACTIONS BETWEEN CREEP AND LOW CYCLE FATIOUE IN A NICKEL BASE SUPERALLOY. Acta Metall Sin, 1979, 15(4): 518-592.

Download:  PDF(1381KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A trial of creep combined with stress controlled low cycle fatigue has beentested for a nickel base superalloy. The life of the notched specimens in the com-bined test did not always obey the linear cumulative damage law, owing to inter-acting between creep and fatigue. The strongest interactions occurred at 650℃,where the creep ductility of the alloy seemed to be minimum. If the specimens un-derwent certain heat treatment to improve their creep ductility, the interaction dis-appeared. However, no interaction was observed in plain specimens tested at 650℃.According to the fractography and creep ductility of the alloy, the probable causeof the interaction between creep and fatigue has been analyzed.
Received:  18 April 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I4/518

[1] ASME, Interpretation of ASME Boiler and Pressure Vessel Code, Case 1331-5, 1972, p. 387.
[2] Ellison, E. G. and Walton, D., International Conference on Creep and Fatigue in Elevated Temperature Applications, Philadelphia, 1973, p. 173.
[3] Lagneborg, R. and Attermo, R., Met. Trans., 2 (1971) , 1821.
[4] Polhemus, J. F., Spaeth, C. E. and Vogel, W. H., Fatigue at Elevated Temperatures, Amer. Soc. Test. Mater., Spec. Tech. Publ. №. 520, 1973, p. 625.
[5] Vinter, A. and Wilbers, L. G., J. Metals, 22 (1970) , №. 5, 46.
[6] Weize, D. A., Symposium on Creep-Fatigue Interaction, Edited by R. M. Curran, ASME-MPC-3, New York, 1976, p. 25.
[7] Wundt, B. M., Effect of Notches on Low-Cycle Fatigue, Amer. Soc. Test. Mater., Spec. Tech. Publ. №. 490, 1972, p. 5.
[8] Manson, S. S., Fatigue at Elevated Temperatures, Amer. Soc. Test. Mater., Spec. Tech. Publ. №. 520, 1973, p. 744.
No related articles found!
No Suggested Reading articles found!