PREDICTION OF THE PROBABILITY OF SPHEROIDIZATION IN NODULAR CAST IRON BY PARAMETRIC DIAGRAM OF CHEMICAL BOND
Wei Yongde Harbin University of Technology
Cite this article: 

Wei Yongde Harbin University of Technology. PREDICTION OF THE PROBABILITY OF SPHEROIDIZATION IN NODULAR CAST IRON BY PARAMETRIC DIAGRAM OF CHEMICAL BOND. Acta Metall Sin, 1979, 15(4): 559-562.

Download:  PDF(237KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  So far the selection of a proper spheroidizing agent for nodular cast ironproduction is deduced from the experience. On the basis of the related theoriesof chemical bond an attempt was made to suggest a parametric diagram of chemi-cal bond concerning interaction between graphitic carbon and other atoms in mol-ten cast iron. Three distinguishable regions as spheroidizing, transitional and anti-spheroidizing may be designated. The element distribution in either spheroidizingor anti-spheroidizing region appears to agree fairly well with both experimentsand production practice. Furthermore, a function ρ_i has been taken as the measureof probability of spheroidization for certain elements in the spheroidizing region.
Received:  18 April 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I4/559

[1] 陈念贻,键参数函数及其应用,科学出版社,1976,p.1.
[2] 戴安邦等,无机化学教程,人民教育出版社,1972,p.513.
No related articles found!
No Suggested Reading articles found!