A TITANIUM CARBOSULPHIDE PHASE IN ALLOY STEELS AND SUPERALLOYS
Zhang Jushui;Chen Jiaguang Research Institute of Daye Steel Works
Cite this article: 

Zhang Jushui;Chen Jiaguang Research Institute of Daye Steel Works. A TITANIUM CARBOSULPHIDE PHASE IN ALLOY STEELS AND SUPERALLOYS. Acta Metall Sin, 1980, 16(2): 159-256.

Download:  PDF(2928KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The morphology, optical characteristics and composition of a titanium carbo-sulphide phase ccurred in certain low-alloy steels, stainless steels and superalloyshave been investigated by optical icroscopy, TEM and EPMA. Its crystallinestructure has been identified by selected-area electron diffraction echnique. Depend-ing on the mechanism of formation, this phase exhibits two different growthhabits: latelets formed directly from the molten alloy are distributed at cast grainboundries, while very thin aminae were precipitated at austenitic grain bound-aries during cooling from a high temperature. It appears hat the amount of thisbrittle phase in the alloys can be greatly diminished by the addition of smallamounts f rare-earth elements. The composition of this phase is found as:(Ti_(1-m)X_m)_2S(C_(1-n)N_n)
Received:  18 February 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I2/159

[1] Novak, C. J. and Diran, L. M., J. Metals, 15 (1963) , 200.
[2] Little, J. H. and Henderson, J. J. M., Effect of Second Phase Particles on the Mechanical Properties of Steel, Iron and Steel Inst., London, 1971, p. 182.
[3] Collins, H. E. and Quigg, R. J., ASM Trans. Quart. 61 (1968) , 139.
[4] Wallace, W., Holt, R. T. and Terada, T., Metallography, 6 (1973) , 511.
[5] Kudielka, H. and Rohde, H., Z. Kristallogr. Kristallgeometrie, Kristallphys. Kristallchem., 114(1960) , 447.
[6] da CASA, C. and Nileshwar, V. B., J. Iron Steel Inst., 207 (1969) , 1003.
[7] Brown, J. F., Clark, W. D. and Parker, A., Metallurgia, 56 (1957) , 215.
[8] Walter Koch, Metallkundliche Analyse, Verlag Stahleisen GmbH., Dusseldorf und Verlag Chemie, GmbH, Weinheim/Bergstr., 1965, pp. 237--238.
[9] 冶金工业部钢铁研究院主编,合金钢手册,上册,第一分册,中国工业出版社,北京,1971,p.106.
[10] 成田贵一,松 本洋,铁钢,58(1972) ,1930.
[11] 成田贵一,日本金属学会会报,7(1968) ,742.
[12] 郭可信,金属学报,14(1978) ,73.
[13] Wyckoff, R. W. G., Crystal Structures, 2nd Edition, Vol. 1, Interscience Publishers, New York, 1963, pp. 146--148.
[14] #12~
No related articles found!