A TITANIUM CARBOSULPHIDE PHASE IN ALLOY STEELS AND SUPERALLOYS |
Zhang Jushui;Chen Jiaguang Research Institute of Daye Steel Works |
|
Cite this article:
Zhang Jushui;Chen Jiaguang Research Institute of Daye Steel Works. A TITANIUM CARBOSULPHIDE PHASE IN ALLOY STEELS AND SUPERALLOYS. Acta Metall Sin, 1980, 16(2): 159-256.
|
Abstract The morphology, optical characteristics and composition of a titanium carbo-sulphide phase ccurred in certain low-alloy steels, stainless steels and superalloyshave been investigated by optical icroscopy, TEM and EPMA. Its crystallinestructure has been identified by selected-area electron diffraction echnique. Depend-ing on the mechanism of formation, this phase exhibits two different growthhabits: latelets formed directly from the molten alloy are distributed at cast grainboundries, while very thin aminae were precipitated at austenitic grain bound-aries during cooling from a high temperature. It appears hat the amount of thisbrittle phase in the alloys can be greatly diminished by the addition of smallamounts f rare-earth elements. The composition of this phase is found as:(Ti_(1-m)X_m)_2S(C_(1-n)N_n)
|
Received: 18 February 1980
|
[1] Novak, C. J. and Diran, L. M., J. Metals, 15 (1963) , 200. [2] Little, J. H. and Henderson, J. J. M., Effect of Second Phase Particles on the Mechanical Properties of Steel, Iron and Steel Inst., London, 1971, p. 182. [3] Collins, H. E. and Quigg, R. J., ASM Trans. Quart. 61 (1968) , 139. [4] Wallace, W., Holt, R. T. and Terada, T., Metallography, 6 (1973) , 511. [5] Kudielka, H. and Rohde, H., Z. Kristallogr. Kristallgeometrie, Kristallphys. Kristallchem., 114(1960) , 447. [6] da CASA, C. and Nileshwar, V. B., J. Iron Steel Inst., 207 (1969) , 1003. [7] Brown, J. F., Clark, W. D. and Parker, A., Metallurgia, 56 (1957) , 215. [8] Walter Koch, Metallkundliche Analyse, Verlag Stahleisen GmbH., Dusseldorf und Verlag Chemie, GmbH, Weinheim/Bergstr., 1965, pp. 237--238. [9] 冶金工业部钢铁研究院主编,合金钢手册,上册,第一分册,中国工业出版社,北京,1971,p.106. [10] 成田贵一,松 本洋,铁钢,58(1972) ,1930. [11] 成田贵一,日本金属学会会报,7(1968) ,742. [12] 郭可信,金属学报,14(1978) ,73. [13] Wyckoff, R. W. G., Crystal Structures, 2nd Edition, Vol. 1, Interscience Publishers, New York, 1963, pp. 146--148. [14] #12~ |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|