Abstract The process of opposite martensite transformation in Ni32Co4Cu alloy on heating has been studied. The stabilization and super-stabilization of austenite may be sufficiently displayed by the phase change cold work for austenite in the opposite transformation. After the double deep cold cyclic treatment, an alloy of lower linear expansion coefficient and stable microstructure under low temperature was obtained, as well as it was available to improve its mechanical properties and machinability.
|
|