Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (2): 221-251    DOI:
Current Issue | Archive | Adv Search |
STABILIZATION AND SUPER-STABILIZATION OF AUSTENITE DURING OPPOSITE MARTENSITE TRANSFORMATION IN CERTAIN Fe-Ni BASE ALLOY
Chen Sen
Cite this article: 

Chen Sen. STABILIZATION AND SUPER-STABILIZATION OF AUSTENITE DURING OPPOSITE MARTENSITE TRANSFORMATION IN CERTAIN Fe-Ni BASE ALLOY. Acta Metall Sin, 1981, 17(2): 221-251.

Download:  PDF(1661KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The process of opposite martensite transformation in Ni32Co4Cu alloy on heating has been studied. The stabilization and super-stabilization of austenite may be sufficiently displayed by the phase change cold work for austenite in the opposite transformation. After the double deep cold cyclic treatment, an alloy of lower linear expansion coefficient and stable microstructure under low temperature was obtained, as well as it was available to improve its mechanical properties and machinability.
Received:  18 February 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I2/221

No related articles found!
No Suggested Reading articles found!