Abstract The binary A-15 phases formation and their T_c variation have been studied by means of the bond-parametric diagram. It was ascertained that the A-15 phases locate in a definite region on the plot of electron density e/a vs radii ratio of components r_A/r_B. The A-15 phase cannot form any longer for the ratio r_A/r_B over a certain critical value which varies with e/a periodically. On the plot, the T_c distribution of A-15 Phases is shown with regularity. The A-15 phases with T_c higher than 1, 4.2, 10, 15 or 20 K are concentrated in the regions of corresponding isotherms. The ratio r_A/r_B, and e/a as well, may be important parameters in determining T_c. As compared with Matthias' rule, a better result in determining the location of A-15 phases of high T_c has been obtained by the consideration of both factors.
|
|
Received: 18 February 1981
|
[1] Matthias, B. T., Phys. Today, 24 (1971) , № 8, 23. [2] Hartsough, L. D., J. Phys. Chem. Solid, 45 (1974) , 1691. [3] 陈念贻,中国科学,1974,№ 6,580. [4] Testardi, L. R., Rev. Mod. Phys., 47 (1975) , 637. [5] Roberts, B. W., J. Phys. Chem. Ref. Data., 5 (1976) , 581. [6] #1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|