Acta Metall Sin  1981, Vol. 17 Issue (2): 225-227    DOI:
Current Issue | Archive | Adv Search |
AN EMPIRICAL RULE OF BINARY A-15 PHASES FORMATION AND THEIR T_c VARIATION
Shi Tiansheng; Zhang Hong and Zheng Longru (Shanghai Institute of Metallurgy; Academia Sinica)
Cite this article: 

Shi Tiansheng; Zhang Hong and Zheng Longru (Shanghai Institute of Metallurgy; Academia Sinica). AN EMPIRICAL RULE OF BINARY A-15 PHASES FORMATION AND THEIR T_c VARIATION. Acta Metall Sin, 1981, 17(2): 225-227.

Download:  PDF(225KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The binary A-15 phases formation and their T_c variation have been studied by means of the bond-parametric diagram. It was ascertained that the A-15 phases locate in a definite region on the plot of electron density e/a vs radii ratio of components r_A/r_B. The A-15 phase cannot form any longer for the ratio r_A/r_B over a certain critical value which varies with e/a periodically. On the plot, the T_c distribution of A-15 Phases is shown with regularity. The A-15 phases with T_c higher than 1, 4.2, 10, 15 or 20 K are concentrated in the regions of corresponding isotherms. The ratio r_A/r_B, and e/a as well, may be important parameters in determining T_c. As compared with Matthias' rule, a better result in determining the location of A-15 phases of high T_c has been obtained by the consideration of both factors.
Received:  18 February 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I2/225

[1] Matthias, B. T., Phys. Today, 24 (1971) , № 8, 23.
[2] Hartsough, L. D., J. Phys. Chem. Solid, 45 (1974) , 1691.
[3] 陈念贻,中国科学,1974,№ 6,580.
[4] Testardi, L. R., Rev. Mod. Phys., 47 (1975) , 637.
[5] Roberts, B. W., J. Phys. Chem. Ref. Data., 5 (1976) , 581.
[6] #1