A FORMULA FOR γ′-PHASE AMOUNTING IN PRECIPITATION HARDENING NICKEL-BASE SUPERALLOYS
Yang Hongcai (Northeast Institute of Technology; Shenyang) (Manuscript received 13 April; 1981)
Cite this article: 

Yang Hongcai (Northeast Institute of Technology; Shenyang) (Manuscript received 13 April; 1981). A FORMULA FOR γ′-PHASE AMOUNTING IN PRECIPITATION HARDENING NICKEL-BASE SUPERALLOYS. Acta Metall Sin, 1982, 18(4): 510-514.

Download:  PDF(330KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A formula for calculation of the possible wt-% content of γ'-phase, G(γ'), formed in the precipitation hardening nickel-base superalloys was derived as: G(γ')=6.662C_(al)+4.256C(Ti)+2.896C_(Nb)+2.153C_V+1.973C_(Ta) +0.905C_W+0.393C_(Mo)+0.121C_(Cr)+0.001C_(Co) where C with sub-symbol of an alloying element is its own wt-% contained in such superalloy. The calculation for 25 commercial nickel-base superalloys was made by this formula with satisfactory results.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/510

1 Woodyatt, L.R.; Sims, C.T.; Beattie, H.J., Trans. Metall. Soc. AIME, 236(1966) , 519.
2 Dreshfieid, R.L.; Wallace, J.F., NASA-CR-120 940,(1972) ,P.134.
3 Krige, O.H., ASM Trans. Q., 62(1969) , 195.
4 渡辺力藏,九重常男,铁鋼,61(1975) ,2277.
5 Watanabe, R.; Kuno, T., Trans. Iron Steel Inst. Jpn., 16(1976) , 439.
6 Decker, R.F.; Sims, C.T., The Superalloys, Eds. Sims, C.T.; Hagel, W.C., Wiley New York, 1972, p.33.
7 #12
8 #12
No related articles found!
No Suggested Reading articles found!