A NOTE ON CARBIDE PRECIPITATION IN Fe-Si-C ALLOY
Tao Zhengxing Xiao Jimei Hsiao Chi-mei Zhu Fengwu (Beijing University of Iron and Steel Technology) (Manuscript received 12 October; 1981)
Cite this article: 

Tao Zhengxing Xiao Jimei Hsiao Chi-mei Zhu Fengwu (Beijing University of Iron and Steel Technology) (Manuscript received 12 October; 1981). A NOTE ON CARBIDE PRECIPITATION IN Fe-Si-C ALLOY. Acta Metall Sin, 1982, 18(4): 507-526.

Download:  PDF(1317KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was conducted to obtain a better understanding of carbide precipitation occurring in a cold-rolled commercial 3%Si-Fe sheet after 900℃ 1 h solid solution treatment by TEM observation. It was shown that under different aging conditions two carbides, namely ε-carbide and cementite Fe_3C, may be precipitated by either intragranular or intergranular mode. While the orientation of the intergranular precipitation of Fe_3C under elevated temperature seems to be a Bagaryatskii’s relatioship between itself and one of the matrix grains.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/507

1 Leslie, W.C., Trans. ASM, 53(1961) , 715.
2 Keh, A.S.; Leslie, W.C., Materials Science Research, Vol. 1, Eds. Stadelmaier, H.H.; Austin, W.W., Plenum Press, New York, 1963, p.208.
3 Speich, G.R.; Leslie, W,C., Metall. Trans., 3(1972) , 1043.
4 Langer, F.W., Met. Sci.J., 2(1968) , 59.
5 Leslie, W.C., Acta Metall., 9(1961) , 1004.
6 Wangenblast, H.W.; Clenn, R., Metall. Trans., 1(1970) , 2299.
7 李春志,物理学报,28(1979) ,314.
8 #12
No related articles found!
No Suggested Reading articles found!