Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (4): 515-518    DOI:
Current Issue | Archive | Adv Search |
INTERACTION BETWEEN HYDROGEN AND A TYPE Ⅲ CRACK
Chu Wuyang Xiao Jimei Hsiao Chi-mei Wang Cheng Zhu Shuyan (Beijing University of Iron and Steel Tecnology) (Manuscript received 26 September; 1981)
Cite this article: 

Chu Wuyang Xiao Jimei Hsiao Chi-mei Wang Cheng Zhu Shuyan (Beijing University of Iron and Steel Tecnology) (Manuscript received 26 September; 1981). INTERACTION BETWEEN HYDROGEN AND A TYPE Ⅲ CRACK. Acta Metall Sin, 1982, 18(4): 515-518.

Download:  PDF(441KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  For a charged type Ⅲ cracked or notched specimens of ultra-high strength steels, the hydrogen induced delayed cracking(HIDC)could occur along the planes inclined 3π/4 to a plane normal to the torsion axis. No delayed cracking and failure occurred in a uncharged or outgased type Ⅲ specimen and a flat shear fracture would be obtained on the plane normal to the torsion axis. The calculation shows that the interaction energy between shear stress field of tye type Ⅲ crack and the strain field of an interstitial hydrogen atom has a minimum value on the planes inclined 3π/4 to the plane normal to the torsion axis. Hence, atomic hydrogen will diffuse to and be enriched in these planes and HIDC will occur along these planes.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/515

1 褚武扬;肖纪美;李世琼;朱淑彦,金属学报,18(1981) ,47.
2 褚武扬;肖纪美;李世琼,金属学报,17(1981) ,10.
3 Chu,W.Y.(褚武扬);Hsiao,C.M.(肖纪美),Li,S.Q.(李世琼),Corrosion,36(1980) ,475;37 (1981) ,320.
4 Cochardt, A.U.; Schock, G.; Wiedersich, H., Acta Metall., 3(1955) , 533.
No related articles found!
No Suggested Reading articles found!