Acta Metall Sin  1983, Vol. 19 Issue (2): 73-78    DOI:
Current Issue | Archive | Adv Search |
FRACTURE TOUGHNESS OF A CAST Mg ALLOY ZM5
WANG Chang; GAO Daxing; HU Yu (Huazhong University of Science and Technology; Wuhan)
Cite this article: 

WANG Chang; GAO Daxing; HU Yu (Huazhong University of Science and Technology; Wuhan). FRACTURE TOUGHNESS OF A CAST Mg ALLOY ZM5. Acta Metall Sin, 1983, 19(2): 73-78.

Download:  PDF(1327KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fracture toughness was determined for various thickness, B=20—120mm, of compact tension specimens of a cast Mg alloy ZM5 according to ASTM E399—78. A proposal could be thus made to the relaxation of P_(max)/P_Q from≤1.1 to ≤1.6 for this alloy.
Received:  18 February 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I2/73

1 Standard of Test for Plane Strain Fracture Toughness of Materials, ASTM E 399-78, 1978.
2 YB 947-78,金属材料平面应变断裂韧性K_(Ie)试验方法.
3 中山大学物理系断裂韧性组,未发表资料.
4 冯师颜,误差理论与实验数据处理,科学出版社,1964,p.21,56.
5 刘文挺,固体力学学报,1(1981) ,92.
6 北京钢铁研究院金属物理室,工程断裂力学,上册,国防工业出版社,1977,p.394.Y
No related articles found!